Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 4.10 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 4.10 - 18.7 GPa
595 - 2710 ksi
Average value: 15.1 GPa Grade Count:26
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Modulus of Elasticity 4.10 - 8.64 GPa
595 - 1250 ksi
Average value: 7.00 GPa Grade Count:5
Overview of materials for Phenolic; Unreinforced; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of..
Modulus of Elasticity 4.10 - 20.0 GPa
595 - 2900 ksi
Average value: 14.3 GPa Grade Count:24
Overview of materials for Nylon 12, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Modulus of Elasticity 4.10 GPa
595 ksi
Sample Type 1B, 50 mm/min; ISO 527-1/2:1993
Global EPP PA 6C MOLY Cast Polyamide 6 + MoS2
Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of ..
Modulus of Elasticity 4.10 GPa
595 ksi
std. dev. 0.55 GPa
Schmelzer Industries Pearlveil 110-10 Fiberglass Veil
Economical alternative for flat or shallow applications. Suitable for hand lay-up, pre-form molding, press molding, vacuum molding, and injection molding. Data provided by the manufacturer, Schmel..
Modulus of Elasticity 4.10 GPa
595 ksi
ISO 178
Addiplast Addilene J 420 K24 Polypropylene Copolymer
High densityInformation provided by Addiplast.
Modulus of Elasticity 4.10 - 11.0 GPa
595 - 1600 ksi
Average value: 8.69 GPa Grade Count:7
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma..
Modulus of Elasticity 4.10 - 4.50 GPa

@Temperature 60.0 - 150 °C
595 - 653 ksi

@Temperature 140 - 302 °F
Average value: 4.33 GPa Grade Count:1
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a..
Modulus of Elasticity 4.10 - 13.1 GPa
595 - 1900 ksi
Average value: 8.77 GPa Grade Count:19
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..
Copyright © lookpolymers.com All Rights Reserved