Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 204 GPa @Temperature 200 °C |
29600 ksi @Temperature 392 °F |
|
Haynes 214® alloy sheet Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Modulus of Elasticity | 204 GPa @Temperature 200 °C |
29600 ksi @Temperature 392 °F |
|
Haynes 214® alloy, 0% cold reduction Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Modulus of Elasticity | 204 GPa @Temperature 200 °C |
29600 ksi @Temperature 392 °F |
|
Haynes 214® alloy, 10% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Modulus of Elasticity | 204 GPa @Temperature 200 °C |
29600 ksi @Temperature 392 °F |
|
Haynes 214® alloy, 20% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Modulus of Elasticity | 204 GPa @Temperature 200 °C |
29600 ksi @Temperature 392 °F |
|
Haynes 214® alloy, 20% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Modulus of Elasticity | 204 GPa @Temperature 200 °C |
29600 ksi @Temperature 392 °F |
|
Haynes 214® alloy, 30% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Modulus of Elasticity | 204 GPa @Temperature 200 °C |
29600 ksi @Temperature 392 °F |
|
Haynes 214® alloy, 40% cold reduction Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Modulus of Elasticity | 204 GPa @Temperature 200 °C |
29600 ksi @Temperature 392 °F |
|
Haynes 214® alloy, 50% cold reduction Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Modulus of Elasticity | 204 GPa @Temperature 200 °C |
29600 ksi @Temperature 392 °F |
|
Haynes 214® alloy, 50% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Modulus of Elasticity | 204 GPa @Temperature 200 °C |
29600 ksi @Temperature 392 °F |
|
Haynes 214® alloy, sheet, 100 hours exposure at 760°C (1400°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Modulus of Elasticity | 204 GPa @Temperature 200 °C |
29600 ksi @Temperature 392 °F |
|
Haynes 214® alloy, sheet, 100 hours exposure at 980°C (1800°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Modulus of Elasticity | 204 GPa @Temperature 200 °C |
29600 ksi @Temperature 392 °F |
|
Haynes 214® alloy, sheet, 1000 hours exposure at 980°C (1800°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Modulus of Elasticity | 204 GPa @Temperature 300 °C |
29600 ksi @Temperature 572 °F |
|
Haynes 25 alloy, cold worked sheet, 20% cold reduction, aged at 370°C (700°F) for 1 hour Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Modulus of Elasticity | 204 GPa @Temperature 300 °C |
29600 ksi @Temperature 572 °F |
|
Haynes 25 alloy, cold worked sheet, 20% cold reduction, aged at 595°C (1100°F) for 2 hours Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Modulus of Elasticity | 204 GPa @Temperature 300 °C |
29600 ksi @Temperature 572 °F |
|
Haynes 25 alloy, hot rolled and 1230°C solution annealed sheet Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Modulus of Elasticity | 204 GPa @Temperature 150 °C |
29600 ksi @Temperature 302 °F |
|
Haynes HR-160® alloy plate, aged 4000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Modulus of Elasticity | 204 GPa @Temperature 150 °C |
29600 ksi @Temperature 302 °F |
|
Haynes HR-160® alloy, plate, aged 4000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Modulus of Elasticity | 204 GPa @Temperature 150 °C |
29600 ksi @Temperature 302 °F |
|
Haynes HR-160® alloy, plate, aged 8000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Modulus of Elasticity | 204 GPa @Temperature 300 °C |
29600 ksi @Temperature 572 °F |
|
Haynes 25 alloy, cold worked sheet, 15 % cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Modulus of Elasticity | 204 GPa @Temperature 300 °C |
29600 ksi @Temperature 572 °F |
|
Haynes 25 alloy, room temperature after 20% cold reduction, 1175°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Modulus of Elasticity | 204 GPa @Temperature 300 °C |
29600 ksi @Temperature 572 °F |
|
Haynes 25 alloy, sheet Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Modulus of Elasticity | 204 GPa @Temperature 300 °C |
29600 ksi @Temperature 572 °F |
|
Haynes 25 alloy, vacuum investment castings, solution treated Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Modulus of Elasticity | 204 GPa | 29600 ksi | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Round Tensile strength (ultimate and yield), hardness, impact, and elongation values reported here are typical for Age Hardened Round samples. Other property values are typical of INCONEL® alloy 725.D.. |
|||
Modulus of Elasticity | 204 GPa | 29600 ksi | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Tube Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Age Hardened Tube samples. Other property values are typical of INCONEL® alloy 725.Data provi.. |
|||
Modulus of Elasticity | 204 GPa | 29600 ksi | |
California Fine Wire Nickel A 200 Nickel Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Modulus of Elasticity | 204 GPa | 29600 ksi | |
Carpenter Pyrowear® 675 Stainless Steel, Tempered 510°C, Longitudinal Properties Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c.. |
|||
Modulus of Elasticity | 204 GPa @Temperature 300 °C |
29600 ksi @Temperature 572 °F |
|
Haynes 25 alloy, room temperature after 15% cold reduction, 1120°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |
|||
Modulus of Elasticity | 204 GPa @Temperature 300 °C |
29600 ksi @Temperature 572 °F |
|
Haynes 25 alloy, room temperature after 15% cold reduction, 1175°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |
|||
Modulus of Elasticity | 204 GPa @Temperature 300 °C |
29600 ksi @Temperature 572 °F |
|
Haynes 25 alloy, room temperature after 20% cold reduction, 1065°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |
|||
Modulus of Elasticity | 204 GPa @Temperature 300 °C |
29600 ksi @Temperature 572 °F |
|
Haynes 25 alloy, room temperature after 15% cold reduction, 1065°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |