Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.90 GPa | 421 ksi | ASTM D638 |
Plaskolite Optix® CA-51 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Medium heat resistance and medium flow. |
|||
Modulus of Elasticity | 2.90 - 12.4 GPa | 420 - 1790 ksi | Average value: 8.85 GPa Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum va.. |
|||
Modulus of Elasticity | 2.90 - 7.00 GPa | 420 - 1020 ksi | Average value: 4.13 GPa Grade Count:21 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Modulus of Elasticity | 2.90 - 5.30 GPa @Temperature 60.0 - 90.0 °C |
421 - 769 ksi @Temperature 140 - 194 °F |
Average value: 4.05 GPa Grade Count:2 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Modulus of Elasticity | 2.90 - 12.0 GPa | 421 - 1740 ksi | Average value: 6.04 GPa Grade Count:155 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Modulus of Elasticity | 2.90 - 23.0 GPa | 420 - 3340 ksi | Average value: 12.2 GPa Grade Count:27 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Modulus of Elasticity | 2.90 GPa | 421 ksi | |
Lehmann & Voss LUVOCOM® 19-7744 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Modulus of Elasticity | 2.90 GPa | 421 ksi | ISO 527-1 |
Dow BETAMATE™ XW 1044-3 Epoxy BETAMATE™ XW 1044-3 is a one component, epoxy based adhesive especially developed for the body shop. The adhesive can be applied by robot systems and it shows high adhesion to metal and non-metal .. |
|||
Modulus of Elasticity | 2.90 GPa | 421 ksi | Conditioned; ISO 178 |
Addiplast Addilene H 490 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.90 GPa | 421 ksi | ISO 178 |
Addiplast Addilene H 530 N30 Polypropylene Homopolymer Good surface appearanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.90 GPa | 421 ksi | ISO 178 |
Addiplast Addilene H 532 N30 Polypropylene Homopolymer Good surface appearanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.90 GPa | 421 ksi | ISO 178 |
Addiplast Addinyl A2 E Flame Retardant Nylon 66 Flame retardant, halogen freeInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.90 GPa | 421 ksi | ISO 527-1/-2 |
BASF Ultramid® B3ZG3 BK 30564 15% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 15% glass fiber reinforced injection-molding grade, for instance, for automotive cable conduits.Information provided by BASF |
|||
Modulus of Elasticity | 2.90 GPa | 421 ksi | ISO 527-1/-2 |
BASF Ultramid® FRee B3U31G4 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Modulus of Elasticity | 2.90 GPa | 421 ksi | ASTM D638 |
Plaskolite West Optix® CA-51 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Medium heat resistance and medium flow. |
|||
Modulus of Elasticity | 2.90 GPa | 421 ksi | ISO 178 |
Addiplast Addinyl PMD 20104 Nylon 66 High molding rateInformation provided by Addiplast. |