Mechanical Properties Metric English Comments
Modulus of Elasticity >= 0.600 GPa
>= 87.0 ksi
ISO.178 DN.53452
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000
PE 1000: Polyethylene with very high molecular weight (UHMW - PE 1000; Ultra High Molecular Weight Polyethylene). Polyethylenes with molecular weight higher than 3 million gr/mol. POLIPOLEN® PE (P..
Modulus of Elasticity 0.600 - 12.1 GPa
87.0 - 1750 ksi
Average value: 2.43 GPa Grade Count:36
Overview of materials for Nylon 46, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Modulus of Elasticity 0.600 - 8.31 GPa

@Temperature -40.0 - 150 °C
87.0 - 1210 ksi

@Temperature -40.0 - 302 °F
Average value: 3.50 GPa Grade Count:5
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Modulus of Elasticity 0.600 - 12.1 GPa
87.0 - 1750 ksi
Average value: 6.84 GPa Grade Count:104
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
Modulus of Elasticity 0.600 - 41.4 GPa
87.0 - 6000 ksi
Average value: 2.65 GPa Grade Count:125
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Modulus of Elasticity 0.600 GPa
87.0 ksi
ISO R527
Arkema Group Orgalloy® LE 60LMXV Polyamide 6 Alloy
Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
Modulus of Elasticity 0.600 GPa
87.0 ksi
Conditioned; ISO 178
Addiplast Addinyl A2 X Nylon 66
High impact resistanceInformation provided by Addiplast.
Modulus of Elasticity 0.600 GPa
87.0 ksi
Conditioned; ISO 178
Addiplast Addinyl C2 R Nylon 66/6
High impact resistanceInformation provided by Addiplast.
Modulus of Elasticity >= 0.600 GPa
>= 87.0 ksi
ISO.178 DN.53452
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000
PE 1000: Polyethylene with very high molecular weight (UHMW - PE 1000; Ultra High Molecular Weight Polyethylene). Polyethylenes with molecular weight higher than 3 million gr/mol. POLIPOLEN® PE (P..
Modulus of Elasticity 0.600 - 15.4 GPa

@Temperature 60.0 - 175 °C
87.0 - 2230 ksi

@Temperature 140 - 347 °F
Average value: 4.73 GPa Grade Count:5
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..
Copyright © lookpolymers.com All Rights Reserved