Mechanical Properties Metric English Comments
Modulus of Elasticity 0.000600 GPa
0.0870 ksi
10% Modulus, Cured 7 min at 177°C and Post Cured 2 hr at 232°C
DuPont Performance Polymers VTR 8650 (GBL-S) Peroxide Cured Fluoroelastomer (FKM) Formulation
FormulationVTR 8650
Modulus of Elasticity 0.000600 GPa
0.0870 ksi
10% Modulus, Cured 7 min at 177°C and Post Cured 16 hr at 232°C
DuPont Performance Polymers VTR GLT Peroxide Cured Fluoroelastomer (FKM) Formulation
FormulationViton® VTR-8500
Modulus of Elasticity 0.000600 - 9.20 GPa
0.0870 - 1330 ksi
Average value: 0.234 GPa Grade Count:42
Overview of materials for Thermoset Fluoroelastomer
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr..
Modulus of Elasticity 0.000600 GPa
0.0870 ksi
10% Modulus, Cured 7 min at 177°C and Post Cured 2 hr at 232°C
DuPont Performance Polymers VTR 8500 (GLT-S) 8500 Peroxide Cured Fluoroelastomer (FKM) Formulation  (discontin
FormulationViton® GLT