Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Creep Modulus, 1 hour = 450000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 3100 - 3300 MPa
450000 - 479000 psi
Average value: 3230 MPa Grade Count:6
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Tensile Creep Modulus, 1 hour 3100 - 4030 MPa
450000 - 585000 psi
Average value: 3430 MPa Grade Count:4
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Tensile Creep Modulus, 1 hour 3100 MPa
450000 psi
BASF Polystyrol® 143 E Polystyrene (Europe)
Medium strength, easy flowing general-purpose grade, suitable for blending with impact-modified Polystyrol, Styrolux and as a coextruded glossy capping layer.Data was collected by ISO methods and pr..
Tensile Creep Modulus, 1 hour 3100 MPa
450000 psi
BASF Polystyrol® 144 C Polystyrene (Europe)
Very easy flowing grade, often blended with impact-modified Polystyrol or used as a coextruded glossy layer.Data was collected by ISO methods and provided by BASF.
Copyright © lookpolymers.com All Rights Reserved