Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 7200 MPa
1.04e+6 psi
ISO 899-1
Lanxess Pocan® T 7323 000000 PBT + PET, 20% Glass Fiber
PBT+PET, 20% glass fibers, injection molding, improved surface finish, increased temperature peak load
Tensile Creep Modulus, 1 hour 7200 MPa
1.04e+6 psi
ISO 899-1
Lanxess Pocan® T 7323 POS151 000000 PBT + PET, 20% Glass Fiber
PBT+PET, 20% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized
Tensile Creep Modulus, 1 hour 7200 MPa

@Time 3600 sec
1.04e+6 psi

@Time 1.00 hour
ISO 899-1
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8..
Tensile Creep Modulus, 1 hour 7200 - 16500 MPa
1.04e+6 - 2.39e+6 psi
Average value: 11700 MPa Grade Count:8