Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 1800 - 2200 MPa | 261000 - 319000 psi | Average value: 2080 MPa Grade Count:5 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Tensile Creep Modulus, 1 hour | 1800 - 2500 MPa | 261000 - 363000 psi | Average value: 2280 MPa Grade Count:11 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Creep Modulus, 1 hour | 1800 - 2700 MPa | 261000 - 392000 psi | Average value: 2460 MPa Grade Count:9 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Tensile Creep Modulus, 1 hour | 1800 MPa | 261000 psi | |
Arkema Group Oroglas® HFI-7 Acrylic
(discontinued **) OROGLAS HFI-7 is a medium impact grade that in addition to the improvement in impact resistance provides superior flow which contribute to reduce the cycle time and improve demolding.Key features :.. |
|||
Tensile Creep Modulus, 1 hour | 1800 MPa | 261000 psi | |
Covestro Bayblend® T 45 MN Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy, good platable.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sep.. |
|||
Tensile Creep Modulus, 1 hour | 1800 MPa | 261000 psi | |
BASF Polystyrol® 476 L Impact Grade Polystyrene (Europe) Normal flowing, high-impact grade. When extruded it is often mixed with PS 165 H.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Creep Modulus, 1 hour | 1800 MPa | 261000 psi | ISO 899 |
BASF Ultraform H 2320 006 Q600 POM Ultraform H2320 006 is a high-molecular-weight grade of POM for injection molding. It conforms to FDA requirements of 21 CFR 177.2470. |
|||
Tensile Creep Modulus, 1 hour | 1800 MPa | 261000 psi | ISO 899 |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |
|||
Tensile Creep Modulus, 1 hour | 1800 MPa | 261000 psi | |
Arkema Group Oroglas® SG 7 Acrylic, Gamma Radiation Resistant
(discontinued **) OROGLAS SG 7 is special Gamma - radiation - resistant formulation designed for use in medical devises.OROGLAS SG 10 maintains exceptional clarity after 5 megarads of Gamma radiation with no adverse .. |