Polymer Property : Tensile Impact Strength = 111 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 233 kJ/m²

@Temperature -40.0 °C
111 ft-lb/in²

@Temperature -40.0 °F
ASTM D1822
ExxonMobil LL 6235 Injection Molding Resin  (discontinued **)
LL 6235 is a narrow molecular weight butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in ..
Tensile Impact Strength 233 kJ/m²

@Temperature -40.0 °C
111 ft-lb/in²

@Temperature -40.0 °F
ASTM D1822
ExxonMobil LL 6235.19 Injection Molding Resin  (discontinued **)
LL 6235 is a narrow molecular weight butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in ..
Tensile Impact Strength 233 kJ/m²
111 ft-lb/in²
ASTM D1822
Ineos HP55-25-155 HDPE
A high performance high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blowmolding equipment, specifically where applications require ex..
Tensile Impact Strength 233 kJ/m²
111 ft-lb/in²
23°C; ISO 8256/1
DSM Arnitel® EL630 63 Shore D, Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Impact Strength 233 kJ/m²
111 ft-lb/in²
notched, 23°C; ISO 8256/1
DSM Arnitel® EL630 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..