Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 210 kJ/m² | 100 ft-lb/in² | ASTM D1822 |
Network Polymers NPP 50-0252 Description: High Density Polyethylene (HDPE) Blow Molding GradeInformation provided by Network Polymers Inc. |
|||
Tensile Impact Strength | 210 kJ/m² | 100 ft-lb/in² | ASTM D1822 |
Network Polymers Nylon 6609 Description: Natural NylonInformation provided by Network Polymers Inc. |
|||
Tensile Impact Strength | 210 kJ/m² | 100 ft-lb/in² | ASTM D1822 |
Network Polymers Nylon 6609 L Description: Black NylonInformation provided by Network Polymers Inc. |
|||
Tensile Impact Strength | 210 kJ/m² | 100 ft-lb/in² | ASTM D1822 |
ExxonMobil Paxon™ BA50-120 High Density Polyethylene Resin Product Description: BA50-120 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: .. |
|||
Tensile Impact Strength | 210 kJ/m² | 100 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow UNIVAL™ DMDA-6230 NT 7 High Density Polyethylene Resin (HDPE) Good extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6230 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipment to.. |
|||
Tensile Impact Strength | 210 kJ/m² | 100 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow UNIVAL™ DMDD-6200 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDD-6200 NT 7 is a multipurpose polymer designed for the high speed production of blow molded containers used to package hous.. |
|||
Tensile Impact Strength | 210 kJ/m² | 100 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow UNIVAL™ DMDD-6230 NT 7 High Density Polyethylene Resin (HDPE) Good extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDD-6230 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipment to.. |
|||
Tensile Impact Strength | 210 kJ/m² | 100 ft-lb/in² | ASTM D-1822 |
Axiall 3121 Rigid PVC, Extrusion Georgia Gulf 3121 is an exterior grade powder compound formulated for processing applications requiring high production output rate. Having excellent weatherability and impact strength, 3121 is sui.. |
|||
Tensile Impact Strength | 210 kJ/m² | 100 ft-lb/in² | ASTM D-1822 |
Axiall 8302 Rigid PVC, Extrusion & Molding Georgia Gulf 8302 is a clear rigid PVC pellet compound suited for applications where transparency is important in a high sunlight environment. It can be used for exterior transparent profiles such .. |
|||
Tensile Impact Strength | 210 kJ/m² @Temperature -40.0 °C |
100 ft-lb/in² @Temperature -40.0 °F |
ASTM D1822 |
ExxonMobil Paxon™ BC50-100 Sheet Extrusion and Blow Molding Resin
(discontinued **) BC50-100 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Information provided by ExxonMobil .. |