Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 233 kJ/m² @Temperature -40.0 °C |
111 ft-lb/in² @Temperature -40.0 °F |
ASTM D1822 |
ExxonMobil LL 6235 Injection Molding Resin
(discontinued **) LL 6235 is a narrow molecular weight butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in .. |
|||
Tensile Impact Strength | 233 kJ/m² @Temperature -40.0 °C |
111 ft-lb/in² @Temperature -40.0 °F |
ASTM D1822 |
ExxonMobil LL 6235.19 Injection Molding Resin
(discontinued **) LL 6235 is a narrow molecular weight butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in .. |
|||
Tensile Impact Strength | 233 kJ/m² | 111 ft-lb/in² | ASTM D1822 |
Ineos HP55-25-155 HDPE A high performance high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blowmolding equipment, specifically where applications require ex.. |
|||
Tensile Impact Strength | 233 kJ/m² | 111 ft-lb/in² | 23°C; ISO 8256/1 |
DSM Arnitel® EL630 63 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Impact Strength | 233 kJ/m² | 111 ft-lb/in² | notched, 23°C; ISO 8256/1 |
DSM Arnitel® EL630 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |