Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | >= 0.00500 GPa | >= 0.725 ksi | DIN 53504 |
NEXA® PFX8028 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® 45 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound
(discon Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont .. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® 12K85A Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 12K85A is a standard polyester-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be e.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® 12K85LB Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 12K85 LB is a standard polyester-based TPU with a lubricating additive, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mech.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ISO 37 |
Huntsman AVALON® 80 ABU Thermoplastic Polyurethane Introduction: AVALON 80 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 80 ABU is part of the AVALON Perform Range and offers a premi.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | Injection molded parts; ISO 37 |
Huntsman IROGRAN® A 80 H 4826 TPU-Polyester Introduction: IROGRAN A 80 H 4826 is a thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of this product are excellent mechanical properties and hig.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 85 D 5001 DP TPU-Polyester Introduction: IROGRAN A 85 D 5001 DP is a antistatic, polyester based thermoplastic polyurethane intended for extrusion applications and injection molding. IROGRAN A 85 D 5001 DP is part of the HUNT.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | Extruded films: approx. 0.2 mm thickness; ISO 527 |
Lubrizol Advanced Materials Pearlbond® D1160 Thermoplastic Polyurethane Pearlbond™ D1160 is a linear, aromatic polyurethane, supplied in form of small white granules, which combines a high crystallization rate and high thermoplasticity level. Applications: Pearlbo.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® 12F75UV Thermoplastic Polyurethane Elastomer PEARLTHANE® D12F75UV is a UV resistant standard polyester based TPU supplied in form of translucent, colorless or slightly yellowish pellets, featuring a low melting point and very low gel conten.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ISO 37 |
Huntsman AVALON® 80 AB Thermoplastic Polyurethane Introduction: AVALON 75 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 75 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ISO 37 |
Huntsman AVALON® 80 AE Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ISO 37 |
Huntsman AVALON® 80 AHT DP Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLCOAT® 168K Thermoplastic Polyurethane Elastomer PEARLCOAT® 168K is a polyether-based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low-temperature flexibility and very good hydrolysis resistance.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® Clear 15N80 Thermoplastic Polyurethane Elastomer PEARLTHANE® CLEAR 15N80 is a polyether copolymer-based TPU, supplied in form of translucent, colorless, combining low hardness with excellent mechanical properties and excellent hydrolysis resist.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1180 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ISO 37 |
Lubrizol ESTANE® GP80AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 80AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D638 |
ELASTO UK Dryflex® 500850S SEBS Based Material, Unfilled Qualities, 85A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D638 |
ELASTO UK Dryflex® 600900S SEBS Based Material, Filled Qualities, 90A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D638 |
ELASTO UK Dryflex® 660850S SEBS Based Material, Semi-Filled Qualities, 85A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D638 |
ELASTO UK Dryflex® 662850S SEBS Based Material, Semi-Filled Qualities, 85A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D 638 |
API Megol AM DP2395/85 SEBS Adhesion Modified Overmolding for Polar Polymers Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D-638 |
Axiall 8710 Moldings & Extrusions Flexible PVC Low gravity extrusion compound with excellent low temperature properties. Designed for use in weatherstrips and flexible gaskets. Excellent for co-extrusion with rigid PVC.Information provided by .. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D-638 |
Axiall 8740 Moldings & Extrusions Flexible PVC General purpose extrusion compound recommended for use in weatherstrips, screen spline, extruded shapes and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporatio.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D-638 |
Axiall 8743 Moldings & Extrusions Flexible PVC A high quality extrusion compound recommended for weatherstrips, extruded shapes and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D-638 |
Axiall 10703 Wire & Cable Flexible PVC Non-lead stabilized general purpose jacketing compound with good low temperature properties. Recommended for a maximum service temperature of 80°C at a 15 mil wall thickness.Information provided b.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | ASTM D-638 |
Axiall 8741 Moldings & Extrusions Flexible PVC A low gravity general purpose extrusion compound recommended for use in weatherstrips, screen spline, extruded shapes and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axi.. |
|||
100% Modulus | 0.00500 GPa | 0.725 ksi | DIN 53504 |
Lubrizol ESTANE® 54630 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |