Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00470 GPa | 0.682 ksi | ASTM D412 |
Network Polymers Softflex® 7700 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
100% Modulus | 0.00470 GPa | 0.682 ksi | ASTM D412 |
Network Polymers Softflex® 8910 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
100% Modulus | 0.00470 GPa | 0.682 ksi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® HPG-6525 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound
&n Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato.. |
|||
100% Modulus | 0.00470 GPa | 0.682 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 451-87 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant wire and cable elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethy.. |
|||
100% Modulus | 0.00470 GPa | 0.682 ksi | ISO 37 |
Termopol Termoton® K2GA4065A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
100% Modulus | 0.00470 GPa | 0.682 ksi | ASTM D412 |
DuPont Performance Polymers Kalrez® 1058 FFKM Perfluoroelastomer
(discontinued **) A carbon black-filled compound that has been plasticized with perfluorinated oil. It is the softest, lowest modulus compound in the Kalrez line. Generally it is similar in resistance to Compound 1.. |
|||
100% Modulus | 0.00470 GPa | 0.682 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 4180 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4180 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
100% Modulus | 0.00470 GPa | 0.682 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 4480 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4480 is a medium hardness grade possessing exceptional tensile strength, superior compressio.. |
|||
100% Modulus | 0.00470 GPa | 0.682 ksi | DIN 53504 |
Lubrizol ESTANE® 58370 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00470 GPa | 0.682 ksi | Press cure 15 Minutes @ 188°C, Post Cure 24 Hours @ 250°C |
3M Dyneon™ 81TZ High Temperature Perfluoroelastomer 3M™ Dyneon™ PFE 81TZ is a technically advanced high temperature perfluoroelastomer (HT PFE). It is designed to meet the challenges of higher temperature applications. It is classified as FFKM per .. |
|||
100% Modulus | 0.00470 GPa | 0.682 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR Hi-Sil 243 LD Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00470 GPa | 0.682 ksi | ASTM D412 |
Lubrizol Estane® 2102-75A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Memory, elasticity and impact modificationAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane prod.. |
|||
100% Modulus | 0.00470 GPa | 0.682 ksi | ASTM D412/D638 |
Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane Features: It has the highest heat resistance of any Estane TPU resin used in adhesives. Supplied as pale amber granules, it is soluble in THF or THF/MEK blends. Higher heat resistance, tensile and b.. |
|||
100% Modulus | 0.00470 GPa | 0.682 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR Hi-Sil 243 LD Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |