Mechanical Properties Metric English Comments
100% Modulus 0.00276 GPa
0.400 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00276 GPa
0.400 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Mistron Vapor Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00276 GPa
0.400 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00276 GPa
0.400 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N650 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00276 GPa
0.400 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00276 GPa
0.400 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N990 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00276 GPa
0.400 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 64A
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00276 GPa
0.400 ksi
ASTM D412
Huntsman KRYSTALFLEX® PE 193 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
100% Modulus 0.00276 GPa
0.400 ksi
ASTM D412
Teknor Apex UNIPRENE® 7400-64 Thermoplastic Elastomer
Information provided by Teknor Apex Company
100% Modulus 0.00276 GPa
0.400 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00276 GPa
0.400 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 64A
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00276 GPa
0.400 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00276 GPa
0.400 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00276 GPa
0.400 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N650 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00276 GPa
0.400 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00276 GPa
0.400 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00276 GPa
0.400 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N990 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00276 GPa
0.400 ksi
ASTM D638
Colorite Polymers 92-623A General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00276 GPa
0.400 ksi
ASTM D638
Colorite Polymers MULTICHEM™ 6014 Vinyl-Urethane Blend
Description: MULTICHEM™ is characterized by:Greater ResiliencyImproved ElasticityLow Temperature PropertiesLower ExtractabilityMolding and ExtrusionInformation provided by Colorite Polymers.
100% Modulus 0.00276 GPa
0.400 ksi
ASTM D-638
Axiall 8553 Moldings & Extrusions Flexible PVC
A general purpose profile extrusion compound with excellent weathering properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00276 GPa
0.400 ksi
ASTM D412
Advanced Polymer Alloys DURACRYN 8060 NC/BK Thermoplastic Rubber
Information provided by Advanced Polymer Alloys
100% Modulus 0.00276 GPa
0.400 ksi
ASTM D412; ISO 37
Advanced Polymer Alloys DuraGrip™ 6170 BK Melt Processable Elastomer
DuraGrip™ 6170BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6170BK has an excellent soft touch feel a..
100% Modulus 0.00276 GPa
0.400 ksi
ASTM D-638
Axiall 8542 Moldings & Extrusions Flexible PVC
General purpose, flexible PVC compound recommended for extrusion or molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00276 GPa
0.400 ksi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
Advanced Polymer Alloys Alcryn® 2060 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
100% Modulus 0.00276 GPa
0.400 ksi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
Advanced Polymer Alloys Alcryn® 2060 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
100% Modulus 0.00276 GPa
0.400 ksi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
Advanced Polymer Alloys Alcryn® 4660 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
100% Modulus 0.00276 GPa
0.400 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
100% Modulus 0.00276 GPa
0.400 ksi
ASTM D638
Colorite Polymers 6014 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00276 GPa
0.400 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00276 GPa
0.400 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Mistron Vapor Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..