Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00910 GPa | 1.32 ksi | ASTM D412 |
Precision Polymer Engineering Perlast® G60A Perfluoroelastomer A black general purpose perfluoroelastomer compound with excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Suitable for app.. |
|||
100% Modulus | 0.00910 GPa | 1.32 ksi | DIN 53504 |
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
100% Modulus | 0.00910 GPa | 1.32 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 91 P 4945 TPU-Polyester Introduction: IROGRAN A 91 P 4945 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 91 P 4945 is part of the HUNTSMAN technical ext.. |
|||
100% Modulus | 0.00910 GPa | 1.32 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 40 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00910 GPa | 1.32 ksi | |
C.O.I.M. PLAXTER® P 60 Polymeric Plasticizer Description: Formulated with PVC, it is used for the production of fuel pipes, solvents or other oil products.Information provided by P.A.T. Products, Inc. |
|||
100% Modulus | 0.00910 GPa | 1.32 ksi | Press Cure 15 Minutes @ 188°C (370°F), Post Cure 24 Hours @ 250°C (482°F) |
3M Dyneon™ PFE 133TBZ High Temperature Perfluoroelastomer 3M™ Dyneon™ PFE 133TBZ is a technically advanced high temperature perfluorelastomer (HT PFE). It is designed to meet the challenges of higher temperature plasma applications. It is classified as F.. |
|||
100% Modulus | 0.00910 GPa | 1.32 ksi | Press Cure 10 Minutes @ 188°C, Post Cure 16 Hours @ 250°C |
3M Dyneon™ 131TZ High Temperature Perfluoroelastomer 3M™ Dyneon™ 131TZ is a technically advanced high temperature perfluoroelastomer (HT PFE). It is designed to meet the challenges of higher temperature applications. It is classified as FFKM per AST.. |
|||
100% Modulus | 0.00910 GPa | 1.32 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 40 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |