Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00689 GPa | 1.00 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N330 (HAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | 25 mil film; ASTM D412 |
Huntsman IROGRAN® A 85 P 5004 TPU-Polyether IROGRAN® A 85 P 5004 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications.Information provided by Alliance Polymers |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D412-97 |
Saint-Gobain Tygon® R-3400 UV Resistant Tubing Formulation Tygon® R-3400: Ideal for virtually any permanent or temporary chemical transfer application, Tygon® UV Resistant Tubing combines suppleness and flexibility with resistance to a wide range of.. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D412 |
Lubrizol Estane® ALR CL87A Thermoplastic Polyurethane Type: Estane® ALR CL87A is an aliphatic, polycaprolactone-based TPU with a Shore A Durometer of 85-90.Features: Contains a UV package that enhances outdoor weatherability. This high performance re.. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D412 |
Lubrizol Estane® ALR E87A Thermoplastic Polyurethane Type: Estane® ALR E87A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor.. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D412 |
Lubrizol Estane® ALR PC95A Thermoplastic Polyurethane Type: Estane® ALR PC95A is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableAvailable in Americas, Europe, Middle East, Africa, India and Asi.. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N330 (HAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00689 GPa | 0.999 ksi | ASTM D412 |
DuPont Performance Polymers Kalrez® Spectrum™ 6380 Fluoroelastomer DuPont™ Kalrez® Spectrum™ 6380 perfluoroelastomers parts are a non-black product specifically developed for chemical processes involving hot, aggressive amines. In addition, it has excellent over.. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D638 |
Colorite Polymers 7533 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D638 |
Colorite Polymers 7772 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D638 |
Colorite Polymers MULTICHEM™ 8014 Vinyl-Urethane Blend Description: MULTICHEM™ is characterized by:Greater ResiliencyImproved ElasticityLow Temperature PropertiesLower ExtractabilityMolding and ExtrusionInformation provided by Colorite Polymers. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D-638 |
Axiall EX1264 Moldings & Extrusions Flexible PVC General purpose extrusion compound designed for water stop applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D-638 |
Axiall 10801 Wire & Cable Flexible PVC Jacket compound recommended for 80°C maximum service temperature at a minimum wall thickness of 30 mils. UL recognized for 720 hour sunlight resistance.Information provided by Georgia GulfGeorgia .. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D-638 |
Axiall 10805 Wire & Cable Flexible PVC Non-lead stabilized, 75°C rated compound recommended for integral insulation/jacket constructions.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D-638 |
Axiall 18754 Wire & Cable Flexible PVC Non-lead stabilized jacket compound with excellent low temperature performance. Maximum service temperature of 105°C at 40+ mil wall thickness.Information provided by Georgia GulfGeorgia Gulf beca.. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D-638 |
Axiall 18760 Wire & Cable Flexible PVC Non-lead stabilized, matte-finish, jacketing compound with excellent low temperature performance. Maximum 105°C service temperature at 40+ mil. Ideally suited for 90°C applications.Information p.. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D-638 |
Axiall 67441 Wire & Cable Flexible PVC 90°C rated, non-lead stabilized, inner/outer jacketing compound meets -40°C low temp impact and FT4 flame requirements in Teck 90 cables. Low acid gas 12%-13% per CSA test methods. Meets CSA 22... |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D-638 |
Axiall 7810 Moldings & Extrusions Flexible PVC 105°C rated injection molding compound approved for 94 V-0 in black and white at 0.75 mm and also approved for 94 V-0 in all colors at 1.5 mm.Information provided by Georgia GulfGeorgia Gulf became.. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D-638 |
Axiall 8752 Moldings & Extrusions Flexible PVC Low gravity, flame retardant extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D-638 |
Axiall 10757 Wire & Cable Flexible PVC General purpose non-lead stabilized 75°C rated compound recommended for jacketing and general purpose extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporati.. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D-638 |
Axiall 18731 Wire & Cable Flexible PVC Non-lead stabilized, UL recognized 720 hour sunlight resistant in all colors, 105 C rated jacket compound with good low temperature performance.Information provided by Georgia GulfGeorgia Gulf becam.. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D-638 |
Axiall 19740 Wire & Cable Flexible PVC Non-lead stabilized, 105°C rated insulation compound with excellent low temperature properties. Suitable for use in Class 43 applications. Also suitable for injection molding applications.Informa.. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D-638 |
Axiall 19810 Wire & Cable Flexible PVC Primary insulation also recommended for 105°C molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D-638 |
Axiall 491 Wire & Cable Flexible PVC 60°C rated low temperature jacketing compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D-638 |
Axiall 8863 Moldings & Extrusions Flexible PVC A vinyl elastomer extrusion compound with rubber-like properties. Ideally suited for extruded profiles and tubings. Meets the requirements for LP Gas hose per UL21.Information provided by Georgia .. |
|||
100% Modulus | 0.00689 GPa | 1.00 ksi | ASTM D-638 |
Axiall 1701 Clear 7002 Flexible PVC Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |