Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00620 GPa | 0.899 ksi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® 48 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound
(discon Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont .. |
|||
100% Modulus | 0.00620 GPa | 0.899 ksi | Cecilia 20 aged 168 hrs at 175°C |
DuPont Vamac® DP HVA-2 Coagent Test Compound Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper.. |
|||
100% Modulus | 0.00620 GPa | 0.899 ksi | Heat aged 2 weeks at 175°C |
DuPont Vamac® DP Sartomer 350 Coagent Test Compound Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper.. |
|||
100% Modulus | 0.00620 GPa | 0.899 ksi | ASTM D412 |
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane Features: High moisture vapor transmission. Good physical properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and AsiaInf.. |
|||
100% Modulus | 0.00620 GPa | 0.899 ksi | ASTM D412 |
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo.. |
|||
100% Modulus | 0.00620 GPa @Temperature 23.0 °C |
0.899 ksi @Temperature 73.4 °F |
12 months, Weathering @ 45° South, 25 mil - Natural, Shelf |
Lubrizol Estane® 58610 Thermoplastic Polyurethane Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee.. |
|||
100% Modulus | 0.00620 GPa @Temperature 23.0 °C |
0.899 ksi @Temperature 73.4 °F |
12 months, Weathering @ 45° South, 12 mil - Black, Ohio |
Lubrizol Estane® 58610 Thermoplastic Polyurethane Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee.. |
|||
100% Modulus | 0.00620 GPa | 0.899 ksi | ASTM D412 |
UBE UBEPOL VCR617 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
100% Modulus | 0.00620 GPa | 0.899 ksi | ASTM D412 |
Lubrizol Estane® 2355-80AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Damping capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009... |
|||
100% Modulus | 0.00620 GPa | 0.899 ksi | ASTM D412 |
Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane Very good physical properties and hydrolysis resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusionAvailable in Americas, Europe, Middle E.. |
|||
100% Modulus | 0.00620 GPa | 0.899 ksi | DIN 53504 |
Lubrizol ESTANE® 5708F4 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00620 GPa | 0.899 ksi | ISO 37 |
ELASTO UK Dryflex® 5064-101 TPE, Modified Injection Molding Grade for Auto Mud Flaps The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 5064-101 is specifically designe.. |
|||
100% Modulus | 0.00620 GPa | 0.899 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR2102-85AE Polycaprolactone Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
100% Modulus | 0.00620 GPa | 0.899 ksi | ASTM D412 |
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection.. |
|||
100% Modulus | 0.00620 GPa | 0.899 ksi | ASTM D412 |
Lubrizol ESTANE® 58311 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Flat Die/Cast Film Extrusion, Profile ExtrusionAv.. |