Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | >= 0.00400 GPa | >= 0.580 ksi | DIN 53504 |
NEXA® PFX8012 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
100% Modulus | >= 0.00400 GPa | >= 0.580 ksi | DIN 53504 |
NEXA® PFX9014 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
100% Modulus | >= 0.00400 GPa | >= 0.580 ksi | DIN 53504 |
NEXA® PFX9020 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ISO 37 |
Termopol Termoton® V5GA1090A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ISO 37 |
Termopol Termoton® V6GA3075A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.0 PHR Thanecure® ZM MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ISO 527 |
Lubrizol Advanced Materials Pearlbond® 12C75 Thermoplastic Polyurethane Pearlbond® 12C75 is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low softe.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® ECO D12T80 Thermoplastic Polyurethane Type : Pearlthane® ECO D12T80 is a high performance bio-based thermoplastic polyurethane. With ca. 42% bio-based content.Main Application : Injection MouldingSpecial Features : Properties similar.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ISO 37 |
Huntsman AVALON® 75 AE Thermoplastic Polyurethane Introduction: AVALON 75 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 75 AE is part of the AVALON Soft Range and offers a premium soiling material .. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D412 |
Mearthane Durethaneâ„¢ S DS-285A Solid Polyurethane Elastomer TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ISO 527 |
Lubrizol Advanced Materials PEARLBOND® 125/H Linear Thermoplastic Polyurethane Pearlbond™ 125H is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low soft.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | |
Spartech E65350 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1285 Polyester Based TPU Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.0 PHR Thanecure® ZM MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00400 GPa @Temperature 100 °C |
0.580 ksi @Temperature 212 °F |
10 weeks, Heat Resistance |
Lubrizol Estane® 58610 Thermoplastic Polyurethane Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ISO 37 |
Lubrizol ESTANE® GP75AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 75AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | Cecilia 20 aged 168 hrs at 175°C |
DuPont Vamac® DP Activator OC Coagent Test Compound Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
ELASTO UK Dryflex® 660800S SEBS Based Material, Semi-Filled Qualities, 80A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4725P Heat Resistant Molding FormulationNordel® IP 4725P |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 5565 ASTM D3568 FormulationNordel® IP 5565 |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | Vulcanizate, Press cured, TC95 +3min at 180°C |
Dow Nordel® IP 5565 Heat Resistant Peroxide Cured FormulationNordel® IP 5565 |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | Vulcanizate, Press cured, TC95 +3min at 180°C |
Dow Nordel® IP 4570 Heat Resistant Peroxide Compound FormulationNordel® IP 4570 |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 2070 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 4670 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ISO 37 |
AlphaGary Evoprene™ Super G 932 SEBS Thermoplastic Elastomer Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.0 PHR MBT MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1580 Polyester Based TPU Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-2180 Polycaprolactone Based TPU Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |