| Category | Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) |
| Manufacturer | Dow Chemical |
| Trade Name | Nordel® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Dow Nordel® IP 4725P Heat Resistant Molding.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.064 g/cc | 0.03844 lb/in³ | |
| Mooney Viscosity | 48 @Temperature 100 °C |
48 @Temperature 212 °F |
ML 1 + 4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 78 | 78 | Vulcanizate, Press cured, TC95 +3min at 160°C |
| Tensile Strength, Ultimate | 22.0 MPa | 3190 psi | Vulcanizate, Press cured, TC95 +3min at 160°C |
| Elongation at Break | 502 % | 502 % | Vulcanizate, Press cured, TC95 +3min at 160°C |
| 100% Modulus | 0.00400 GPa | 0.580 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
| 200% Modulus | 0.00840 GPa | 1.22 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
| 300% Modulus | 0.0132 GPa | 1.91 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
| Tear Strength | 43.7 kN/m | 249 pli | Die C, Vulcanizate, Press cured, TC95 +3min at 160°C |
| Compression Set | 23 % @Temperature 125 °C |
23 % @Temperature 257 °F |
Pellets cured MDR TC95 + 15 min at 160°C, 70 hr at 125°C; Method B |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -26.0 °C | -14.8 °F | Temperature Retraction, TR-10 |