Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00230 GPa | 0.334 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 181-64 Thermoplastic Rubber
(discontinued **) A black thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be proc.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR Cumar P10 Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N990 (MT) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | ASTM D638 |
Multibase Multi-Flex® TPE A 5904 LC BLK Multi-Flex® LC compounds are a new generation elastomers exhibiting improved compression set at elevated temperature. Multi-Flex® TPE compounds are based on Shell's Kraton G technology and fe.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | ISO 37 |
Kuraray SEPTON® S8004 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | ISO 37 |
Kuraray SEPTON® S8007 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
100% Modulus | 0.00230 GPa | 0.333 ksi | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-60A/B Elastomer KE-1950-60 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | ASTM D412 |
UBE UBEPOL BR360L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N220 (ISAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 5.0 PHR Di-Cup 40C MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | ASTM D412 |
UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR Cumar P10 Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Soft Clay Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N990 (MT) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | |
Lubrizol ESTANE® 5703 Ester Based Thermoplastic Polyurethane Features: Soft compound with high elongation, displays low temperature flexibility and abrasion resistance. It can be processed by means of solution coating, extrusion and melt coating.Uses: Adhesiv.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | ASTM D412/D638 |
Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane Features: High tensile strength, low temperature flexibility, and high adhesion to various substrates such as PET, PVC, and various fabrics.Uses: Fabric coating and audio tape binder, inks and solut.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | ASTM D638 |
ELASTO UK Dryflex® 650700 TPE, Improved Compression Set and High Temperature Resistance, 70A Hardness The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. This grade is designed with improved compressi.. |
|||
100% Modulus | 0.00230 GPa | 0.333 ksi | ASTM D412 |
Advanced Polymer Alloys Alcryn® 2160 BK Melt Processable Rubber Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | 500 mm/min, measured parallel to flow; ISO 37 |
AlphaGary Evoprene™ LF 6151 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Soft Clay Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N220 (ISAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 5.0 PHR Di-Cup 40C MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 101-64 W175 Thermoplastic Rubber
(discontinued **) A black thermoplastic general purpose elastomer designed for thin wall extrusion with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfo.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 281-64 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | ISO 37 |
AlphaGary Evoprene™ 091 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
100% Modulus | 0.00230 GPa | 0.334 ksi | ISO 37 |
AlphaGary Evoprene™ GC 5658 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |