Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00190 GPa | 0.276 ksi | ASTM D412 |
Multibase Multi-Flex® TPE A 6900 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
100% Modulus | 0.00190 GPa | 0.276 ksi | ISO 37 |
Termopol Termoton® K2GA5050A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
100% Modulus | 0.00190 GPa | 0.276 ksi | ISO 37 |
Termopol Termoton® K4GA4055A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
100% Modulus | 0.00190 GPa | 0.275 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00190 GPa | 0.275 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Suprex Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00190 GPa | 0.275 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00190 GPa | 0.275 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 65A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00190 GPa | 0.276 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Polyfil HG90 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00190 GPa | 0.276 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Talc-Mistron Vapor MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00190 GPa | 0.276 ksi | ASTM D412 |
Mearthane Durethaneâ„¢ S DS-260A Solid Polyurethane Elastomer TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
100% Modulus | 0.00190 GPa | 0.276 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 3460 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
100% Modulus | 0.00190 GPa | 0.276 ksi | ASTM D412 |
UBE UBEPOL BR130B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
100% Modulus | 0.00190 GPa | 0.275 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 65A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00190 GPa | 0.276 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N550 (FEF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00190 GPa | 0.276 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Polyfil HG90 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00190 GPa | 0.275 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00190 GPa | 0.275 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Suprex Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00190 GPa | 0.276 ksi | DIN 53504 |
Lubrizol ESTANE® 54660 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | >= 0.00190 GPa | >= 0.276 ksi | ASTM D412 |
3M 755 Hybrid Sealant 3M™ 700-Series Hybrid Sealant and Hybrid Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. They are similar in function as a typical one comp.. |
|||
100% Modulus | >= 0.00190 GPa | >= 0.276 ksi | ASTM D412 |
3M 755FC Hybrid Sealant 3M™ 700-Series Hybrid Sealant and Hybrid Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. They are similar in function as a typical one comp.. |
|||
100% Modulus | 0.00190 GPa | 0.276 ksi | ISO 37 |
AlphaGary Evoprene™ 022 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
100% Modulus | 0.00190 GPa | 0.275 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00190 GPa | 0.276 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N550 (FEF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00190 GPa | 0.275 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00190 GPa | 0.275 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |