Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 45.0 J @Temperature -20.0 °C |
33.2 ft-lb @Temperature -4.00 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Xenoy® 364 PBT This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 45.0 J @Temperature 23.0 °C |
33.2 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Valox® 364 PBT Designed for outdoor telecommunications enclosure applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 45.0 J @Temperature 23.0 °C |
33.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
Diamond Polymers Centrex® 810 Injection Molding Grade Centrex 810 resin is a soft-flow, high-gloss, and medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and .. |
|||
Impact Test | 45.0 J @Thickness 4.00 mm |
33.2 ft-lb @Thickness 0.157 in |
Multi-axial, total energy; ISO 6603-2 |
Azdel Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Impact Test | 45.0 J @Thickness 4.00 mm |
33.2 ft-lb @Thickness 0.157 in |
Multi-axial, total energy; ISO 6603-2 |
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m.. |
|||
Impact Test | 45.0 J @Thickness 4.00 mm |
33.2 ft-lb @Thickness 0.157 in |
Multi-axial, total energy; ISO 6603-2 |
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |