Impact Test 29.8 J

@Temperature -40.0 °C
22.0 ft-lb

@Temperature -40.0 °F
Instrumented Impact, Total Energy; ASTM D3763
ExxonMobil Escorene® LD 722.MV Molding, extrusion and compounding resin  (discontinued **)
Escorene Ultra LD 722.MV is a high vinyl acetate copolymer resin for specialty extrusion and compounding application. Articles made from LD 722.MV are soft and have excellent low temperature toughne..
Impact Test 29.8 J

@Temperature -40.0 °C
22.0 ft-lb

@Temperature -40.0 °F
Instrumented Impact, Total Energy; ASTM D3763
ExxonMobil Escorene® LD 725.21 Molding, extrusion, compounding and adhesive resin  (discontinued **)
Escorene Ultra LD 722.21 is 18 wt% vinyl acetate copolymer suitable for molding, extrusion, compounding and hot melt adhesive applications.Information provided by ExxonMobil Chemical
Impact Test 29.8 J

@Temperature -40.0 °C
22.0 ft-lb

@Temperature -40.0 °F
Instrumented Impact, Total Energy; ASTM D3763
ExxonMobil Escorene® LD 713.93 Molding, extrusion and compounding resin
Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer with very good toughness, high clarity and excellent processability. It is suitable for use in making molded articles, extruded profile..
Impact Test 29.8 J

@Temperature -40.0 °C
22.0 ft-lb

@Temperature -40.0 °F
Instrumented Impact, Total Energy; ASTM D3763
ExxonMobil Escorene® LD 761.36 Molding, extrusion and compounding resin
Escorene Ultra LD 761.36 is a 26.7% vinyl acetate copolymer excellent flexibility and low temperature toughness. LD 761.36 has high filler acceptance.Availability: Latin America, North America and S..
Impact Test 29.8 J

@Temperature -40.0 °C
22.0 ft-lb

@Temperature -40.0 °F
Instrumented Impact, Total Energy; ASTM D3763
ExxonMobil Escorene® LD 783.ND Molding, extrusion and compounding resin  (discontinued **)
Escorene Ultra LD 783.ND is a 33% vinyl acetate copolymer suitable for making a variety of specialty molding and extrusion compounds. It has high clarity and a very low modulus.Information provided ..
Copyright © lookpolymers.com All Rights Reserved