Mechanical Properties Metric English Comments
Impact Test 17.6 J

@Temperature 23.0 °C
13.0 ft-lb

@Temperature 73.4 °F
Multi-Axial, Ductile; ASTM D3763
Flint Hills P9M6K-041A Specialty Impact Copolymer Polypropylene
Features: Good clarity and impact resistance. Product does not contain animal derived components.Applications: Injection molding - durable goodsInformation provided by Flint Hills Resources.
Impact Test 17.6 J

@Temperature 23.0 °C
13.0 ft-lb

@Temperature 73.4 °F
Instrument Impact, Total Energy; ASTM D3763
ExxonMobil OPTEMA™ TC 120 Molding Ethylene Methyl Acrylate
Product Description: Optema TC 120 is an ethylene methyl acrylate copolymer, which can be used as an impact modifier or compatibilizer in polymer compounds. TC 120 has been processed on typical LDPE..
Impact Test 17.6 J

@Temperature 23.0 °C
13.0 ft-lb

@Temperature 73.4 °F
Instrument Impact, Total Energy; ASTM D3763
ExxonMobil Escorene® LD 728.61 Molding, extrusion and compounding resin
Escorene Ultra LD 728.61 is a high vinyl acetate copolymer with low melting temperature and excellent strength properties and toughness.Availability: Latin America, North America and South America A..
Copyright © lookpolymers.com All Rights Reserved