Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 508000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 3500 MPa
508000 psi
McDanel Advanced Ceramics SiAlON
Information provided by McDanel Advanced Ceramic Technologies.
Compressive Strength 3500 MPa
508000 psi
ASTM C-773-88 / DIN 51067T1
CeramTec Rocar® S Silicon Carbide, SSiC
Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch..
Compressive Strength 3500 MPa
508000 psi
ASTM C-773-88 / DIN 51067T1
CeramTec Rocar® SiF Silicon Carbide, SiSiC
Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch..
Compressive Strength 3500 MPa
508000 psi
DIN 51067T1
CeramTec Rocar® SiG Silicon Carbide, SiSiC
Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch..
Compressive Strength 3500 MPa
508000 psi
ASTM C773
CoorsTek Direct Sintered Silicon Carbide, SC DS (SC-30, UltraSiC™)
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Copyright © lookpolymers.com All Rights Reserved