Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.0345 - 0.0621 MPa | 5.00 - 9.00 psi | 0.25 |
Monmouth Rubber & Plastics Durafoamâ„¢ C122A Neoprene/SBR Information provided by Monmouth Rubber & Plastics Corp. |
|||
Compressive Strength | 0.0345 - 0.0621 MPa | 5.00 - 9.00 psi | Deflection @ 25%; ASTM D1056 |
Monmouth Rubber & Plastics Durafoamâ„¢ C42 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Compressive Strength | 0.0345 - 0.0621 MPa | 5.00 - 9.00 psi | 0.25 |
Monmouth Rubber & Plastics Durafoamâ„¢ C42NBR Nitrile Rubber Information provided by Monmouth Rubber & Plastics Corp. |
|||
Compressive Strength | 0.0345 - 0.0621 MPa | 5.00 - 9.00 psi | Deflection @ 25% |
Monmouth Rubber & Plastics Durafoamâ„¢ DK2121 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Compressive Strength | 0.0345 - 0.0896 MPa | 5.00 - 13.0 psi | Deflection @ 25%; ASTM D1056 |
Monmouth Rubber & Plastics Durafoamâ„¢ N207 100% Neoprene Information provided by Monmouth Rubber & Plastics Corp. |
|||
Compressive Strength | 0.0345 - 0.0621 MPa | 5.00 - 9.00 psi | 0.25 |
Monmouth Rubber & Plastics Durafoamâ„¢ P292HD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Compressive Strength | 0.0345 MPa @Temperature 23.0 °C |
5.00 psi @Temperature 73.4 °F |
ASTM D1056 |
Saint-Gobain COHRlastic® R10480 Soft Low Compression Set Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Compressive Strength | 0.0345 MPa | 5.00 psi | Compression Deflection, Value given for 12.7 mm/min, 25% deflection.; ASTM D3574 Test C |
Saint-Gobain Korel® K30-15 Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |
|||
Compressive Strength | 0.0345 MPa | 5.00 psi | 10% deformation |
Unifrax Fiberfrax® 440 Ceramic Fiber Paper 440 paper is a low-cost, high-strength composite paper made from a combination of ceramic fiber, inert fillers, and reinforcing fiberglass. The fiberglass gives added strength to the 440 paper at o.. |
|||
Compressive Strength | 0.0345 MPa | 5.00 psi | 25% deformation |
Unifrax Fiberfrax® Roll Board Ceramic Fiber Paper The lower density, binder chemistry, and bulk ceramic fiber grade used to manufacture Fiberfrax Rollboard paper result in a product with lower cost, higher flexibility, and reduced smoke and odor du.. |
|||
Compressive Strength | 0.0345 MPa | 5.00 psi | 25% deformation |
Unifrax Isofrax® 1260C Paper Fiber Isofrax® 1260C Paper is a unique product which is manufactured by forming Isofrax 1260C Fiber in a nonwoven matrix. The fibers are randomly oriented during manufacture, then held in place with a l.. |
|||
Compressive Strength | 0.0345 MPa | 5.00 psi | 10% Compression, Deflection |
3M Cushion-Mount™ E1115 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Compressive Strength | 0.0345 MPa | 5.00 psi | 10% Compression, Deflection |
3M Cushion-Mount™ E1120 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Compressive Strength | 0.0345 MPa | 5.00 psi | 10% Compression, Deflection |
3M Cushion-Mount™ 1115 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Compressive Strength | 0.0345 MPa | 5.00 psi | 10% Compression, Deflection |
3M Cushion-Mount™ 1120 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Compressive Strength | 0.0345 MPa | 5.00 psi | 10% Compression, Deflection |
3M Cushion-Mount™ 1120K Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Compressive Strength | 0.0345 MPa | 5.00 psi | Compression Deflection, Value given for 12.7 mm/min, 25% deflection.; ASTM D3574 Test C |
Saint-Gobain Korel® K30-20 Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc.. |
|||
Compressive Strength | 0.0345 - 0.0621 MPa | 5.00 - 9.00 psi | 0.25 |
Monmouth Rubber & Plastics Durafoam™ P291HD EPDM Note 1: The Durafoam™100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ¼ i.. |
|||
Compressive Strength | 0.0345 - 0.0621 MPa | 5.00 - 9.00 psi | Deflection @ 25%; ASTM D1056-00 |
Monmouth Rubber & Plastics Durafoam™ PMR 150 EPDM Performance Features: Softness, stiffness & density infinitely variable.High Ozone Resistance. High Ultraviolet Resistance. Non-Staining. Made from Heat Resistant EPDM Non-fogging (plasticizer free.. |