Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | <= 27.6 MPa | <= 4000 psi | Working pressure |
Potters Industries Sphericel® 45P25 Hollow Engineered Glass Microspheres Sphericel® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strength.. |
|||
Compressive Strength | 27.6 MPa | 4000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Fluorosint® 500 PTFE, synthetic mica-filled PTFE, compression molded (ASTM Product Data Sheet) |
|||
Compressive Strength | 27.6 MPa | 4000 psi | 21%, 0.44 w/c w/Tychem 3000 |
Mallard Creek Polymers Tychem® 3100D Yield Modifier Additive Tychem® 3000/3100D is well suited, but not limited to, dry-cast pavers and blocks, SCC, HPC, pre-cast and down hole cementing. Tychem® 3000/3100D is compatible under the most extreme condition.. |
|||
Compressive Strength | 27.6 MPa | 4000 psi | 16%, 0.44 w/c w/Tychem 3000 |
Mallard Creek Polymers Tychem® 3100D Yield Modifier Additive Tychem® 3000/3100D is well suited, but not limited to, dry-cast pavers and blocks, SCC, HPC, pre-cast and down hole cementing. Tychem® 3000/3100D is compatible under the most extreme condition.. |
|||
Compressive Strength | 27.6 MPa | 4000 psi | 1% strain; ASTM D695 |
Saint-Gobain Meldin® 7022 Isostatically Molded Graphite Filled Polyimide Finished parts and basic shapes made from 40% by weight graphite filled polyimide material for applications requiring a low coefficient of thermal expansion, self lubricating properties, and good di.. |
|||
Compressive Strength | >= 27.6 MPa | >= 4000 psi | |
Engineered Syntactic Systems PSF-42 Polyester Subsea Syntactic Void Filler PSF-42 was developed by Navy subcontractors for simple shipyard-based cavity pours of Naval vessels. This system may be used in any free-flood cavity or void, but is especially valuable in difficult.. |
|||
Compressive Strength | 27.6 MPa @Temperature 816 °C |
4000 psi @Temperature 1500 °F |
|
Zircar Ceramics AX-200 Refractory Supported Heater ZIRCAR Refractory Supported Heater Type AX-200 consists of high temperature, helically-wound, iron-chrome-aluminum metallic alloy resistance heating elements fully embedded in a strong, highly stabl.. |
|||
Compressive Strength | 27.6 MPa | 4000 psi | ASTM D695 |
Chesterton ARC 5ES Rapid Repair Stick Description: ARC 5ES is specifically formulated for quick reliable repairs. Its “stick” design combines the performance of a two component system with the convenience of a single component. The AR.. |
|||
Compressive Strength | 27.6 MPa | 4000 psi | |
Cotronics Resbond™ 940 High Temperature Ceramic Adhesive, Fast Set |
|||
Compressive Strength | 27.6 MPa | 4000 psi | Cold Crush Strength |
BNZ Materials Blazecrete 2600 Dense Castable Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as.. |
|||
Compressive Strength | 27.6 MPa | 4000 psi | |
3M HGS4000 Glass Bubbles 3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of.. |
|||
Compressive Strength | 27.6 MPa | 4000 psi | |
3M S38 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Compressive Strength | 27.6 - 41.4 MPa | 4000 - 6000 psi | ASTM C133 |
Ceradyne Thermo-Sil® Castable 120 Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |
|||
Compressive Strength | 27.6 - 41.4 MPa | 4000 - 6000 psi | ASTM C133 |
Ceradyne Thermo-Sil® Castable TG Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |