Mechanical Properties Metric English Comments
Compressive Strength 230 MPa
33400 psi
Pyrotek TS-120 Thermoset Electrical Insulation Product (Nema Grade: GPO-2)
Glass reinforcement, Polyester resin, Cream color. Highly flame resistant. Meets UL 94VO.Information provided by Pyrotek.
Compressive Strength 230 MPa
33400 psi
ASTM D695
Sumitomo Bakelite North America Epiall® 2061B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
Epiall 2061B-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by S..
Compressive Strength 230 MPa

@Treatment Temp. 150 °C,
Time 3600 sec
33400 psi

@Treatment Temp. 302 °F,
Time 1.00 hour
ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Sheets
Description: Electrical and electrotechnical applications. Suitable as high-frequency insulation on account of its dielectric loss. Used as, among other things, an insulation material in large induc..
Compressive Strength 230 MPa

@Temperature 23.0 °C,
Time 86400 sec
33400 psi

@Temperature 73.4 °F,
Time 24.0 hour
50% RH, Axial; ISO 604; IEC/EN 61212-2 5.2
Elektro-Isola G-Etronax EP FR Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes
Description: Mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperatures. Very good stability of electrical properties when exposed to high relati..
Compressive Strength >= 230 MPa
>= 33400 psi
Ambient
China-Yixing Longly Refractories Cordierite Ceramics (Heat Resistance Ceramics)
LONGLY's cordierite ceramics' main crystal phrase is 2MgO-2Al2O2-5SiO2, this composition has low thermal expansion coefficient and excellent thermal shock resistance. Maximum service temperature is..
Compressive Strength 230 MPa
33400 psi
ISO 604
Brandenburger Heavy Duty Mounting Paste
Information provided by Brandenburger Isoliertechnik GmbH&Co.
Compressive Strength 230 MPa
33400 psi
ISO 604
Vyncolit Neopreg Kinel® SK4504 S12 Carbon Reinforced Molding Compound
Epoxy based molding compound long carbon fiber reinforced suited for demanding tribologic applications under dry running conditions, exposed to a wide range of temperatures (-100°C up to 150°C)...
Compressive Strength 230 MPa
33400 psi
Test specimen flat tested; ISO 604
Hexion Bakelite™ PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength
Phenolic molding compound, inorganically filled, glass fiber reinforced, increased mechanical strength, increased temperature stability, low water absorption, good dimensional stability, UL listed m..
Compressive Strength 230 MPa
33400 psi
ASTM D695
Sumitomo Bakelite North America FM 4004F Fiberglass and Mineral Reinforced Phenolic Novolac
FM 4004F is a fiberglass and mineral reinforced phenolic novolac compound with improved strength properties over FM 4004. This compound exhibits excellent dimensional stability and good strength at..