Compressive Strength 208 MPa
30200 psi
ASTM D695
Plenco 4548 Phenolic, Granular, Transfer Molded
PLENCO 04548 is a heat resistant mineral filled phenolic molding compound, offering fast cure rates and hot rigidity. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04548 is avai..
Compressive Strength 208 MPa
30200 psi
ASTM D695
Plenco 5482 Phenolic, Granular, Injection Molded
PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for elect..
Compressive Strength 208 MPa

@Temperature 23.0 °C
30200 psi

@Temperature 73.4 °F
EN ISO 604
Ensinger TECASINT 4021 Polyimide, Black, 15% Graphite (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Compressive Strength 208 MPa
30200 psi
ASTM D695
Plenco 4485 Phenolic, Granular, Transfer Molded
PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a..