Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 121 MPa | 17500 psi | ASTM D695 |
Owens Corning Glass Fiber Reinforced Polystyrene Acrylonitrile (SAN), 20 wt.% glass Polystyrene provides good resistance to alkalis, most organic solvents, weak acids, and household chemicals. It is not recommended for use with strong acids, ketones, esters, and some chlorinated hy.. |
|||
Compressive Strength | 121 MPa | 17500 psi | ASTM D695 |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re.. |
|||
Compressive Strength | 121 MPa | 17500 psi | ASTM D695 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Compressive Strength | 121 MPa | 17500 psi | ASTM D695 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Compressive Strength | 121 MPa | 17500 psi | |
SGL Carbon Group EK 204 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Compressive Strength | 121 MPa | 17500 psi | ASTM D695 |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK) AV-742 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wea.. |
|||
Compressive Strength | 121 MPa | 17500 psi | ASTM D695 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Compressive Strength | 121 MPa | 17500 psi | ASTM D695 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK) KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and.. |
|||
Compressive Strength | 121 MPa | 17500 psi | |
CMT Materials HYTAC® WFT High Temperature, Ultra-Smooth PTFE Impregnated HYTAC-WFT combines the higher temperature, smooth surface properties of HYTAC-WF with PTFE impregnation for low stick surface capability and excellent material distribution. The result is a syntact.. |
|||
Compressive Strength | 121 MPa | 17500 psi | Crosswise; ASTM D635 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Compressive Strength | 121 MPa | 17500 psi | Crosswise; ASTM D635 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Compressive Strength | 121 MPa | 17500 psi | ASTM D695 |
Owens Corning Glass Fiber Reinforced Polyphenylene Oxide (PPO), 20 wt.% glass Polyphenylene Oxide provides excellent resistance to aqueous media. It is softened by aromatic hydrocarbons. Data provided by the manufacturer, Owens Corning. |