Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 96.5 MPa | 14000 psi | ASTM D695 |
PolyOne LubriOne™ NY-10GF/10T BLACK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Compressive Strength | 96.5 MPa | 14000 psi | |
Ohio Carbon Blank OCB EDM-200 Mechanical Grade Graphite Available in a range of sizes and shapes. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series A-100 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series P-0140 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series P-0280 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series Premium 5MM Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series Glass Spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | ASTM D695 |
Oxford Polymers 10GF 10% Glass Fiber Filled Polycarbonate for Injection Molding 10% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Nylatron® MD PA6, Metal-detectable Nylon (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products Broadest size range availability Good mechanical and electrical properties Ideal balance of strength and toughness Cast as finished parts and n.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Nylatron® NSM Nylon, Cast Solid Lubricant Filled, Type 6 (ASTM Product Data Sheet) |
|||
Compressive Strength | 96.5 MPa | 14000 psi | |
Resin Technology Group KONA 877 Low Viscosity, Low Shrinkage, Vacuum Grade Casting Resin Mix ratio 1 to 1 by weight.KONA 877 with HARDENER #112 is a versatile epoxy casting system developed for high performance production potting and encapsulating applications where low shrinkage and ra.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | Break; TM R050-38 |
Resinlab® EP1325LV Thixotropic, Heat Curing Epoxy Adhesive Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where .. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series Premium 1.5MM Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series Premium 2MM Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series Premium 3MM Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | ASTM D695 |
Techmer ES Luriblend® PA6 E ML2 MB Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | 10% strain; ASTM D695 |
Saint-Gobain Meldin® 7001 Direct Formed Polyimide Finished parts and basic shapes made from unfilled polyimide material for structural applications requiring requiring high electrical insulative properties, high purity and low outgassing, and high .. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | ASTM D695 |
Plastics Group Polifil® GFABS-20 20% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | ASTM D695 |
Westlake Plastics Zelux® 10% GF Polycarbonate 10% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Compressive Strength | >= 96.5 MPa | >= 14000 psi | |
Master Bond EP30ND Non-Drip, Dimensionally Stable Epoxy Adhesive Description: Master Bond Polymer System EP30ND is a high viscosity, two component epoxy adhesive/sealant with a paste consistency. It will cure at room temperature or more rapidly at elevated temper.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | Cured |
Atom Adhesives AA-DUCT 902 Epoxy Adhesive and Coating AA-DUCT 902 is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value of.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | cured |
Atom Adhesives AA-DUCT 902LP Epoxy Adhesive AA-DUCT 902LP is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value .. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | cured |
Atom Adhesives AA-DUCT 903 Epoxy Adhesive AA-DUCT 903 is an epoxy adhesive and coating formulation based on Nickel. This epoxy nickel formulation offers the maximum continuity of conductivity with an electrical resistivity value of less tha.. |
|||
Compressive Strength | 96.5 - 124 MPa | 14000 - 18000 psi | |
Bulk Molding Compounds BMC 700 Thermoset Polyester, High Arc Quench Electrical Grade BMC 700 is a general purpose, mineral filled, glass fiber-reinforced polyester compound that was initially designed for molding arc chutes. It has superior arc quench properties. As with all other B.. |
|||
Compressive Strength | 96.5 - 124 MPa | 14000 - 18000 psi | |
Bulk Molding Compounds BMC T12-15526 General Purpose Molding Compound BMC T12-15526 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series A-120 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | Ultimate; TM R050-38 |
Resinlab® EP1046FG Black Electronic Grade Epoxy Encapsulant Resinlab™ EP1046FG Black is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | Ultimate; TM R050-38 |
Resinlab® EP1046FG Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1046FG Clear is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | Break; TM R050-38 |
Resinlab® EP1046FG Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1046FG Clear is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to.. |
|||
Compressive Strength | 96.6 MPa | 14000 psi | |
Henkel Hysol EA 9396/C-2 Paste Adhesive System Two-part, elevated cure, unfilled, low viscosity adhesive with structural properties to 400°F / 204°C.Applications: Structural Repair Low Viscosity Wet Lay-Up Composite Bonding |