Mechanical Properties Metric English Comments
Compressive Strength 8.00 - 12.0 MPa
1160 - 1740 psi
Cold Crushing Strength
Gouda Vuurvast FI 45-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Compressive Strength 8.00 - 12.0 MPa
1160 - 1740 psi
Cold Crushing Strength
Gouda Vuurvast FI 55-11 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Compressive Strength 8.00 - 12.0 MPa
1160 - 1740 psi
Cold Crushing Strength
Gouda Vuurvast FI 65-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Compressive Strength 8.00 MPa
1160 psi
Dried at 110°C (230°F)
Skamol Group SKAMOCAST 14-105 Insulating Castable
SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f..
Compressive Strength 8.00 MPa

@Time 360000 sec
1160 psi

@Time 100 hour
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy
Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor..