Mechanical Properties Metric English Comments
Compressive Strength 74.5 MPa
10800 psi
Flatwise; ASTM D695
Haysite H515 Polyester, High Temp Flex
H515 exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high t..
Compressive Strength 74.5 MPa
10800 psi
Flatwise; ASTM D695
Haysite HTF Polyester, High Temp Flex
HTF exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high te..
Compressive Strength 74.5 MPa
10800 psi
Tra-Con Tra-Cast 3107 Low Shrinkage Epoxy Casting System
TRA-CAST 3107 is a versatile epoxy casting system developed for high performance production potting, encapsulating, casting and tooling applications where low shrinkage, easy handling and flowabilit..