Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 124 - 152 MPa | 18000 - 22000 psi | ASTM D695 |
Mar-Bal MB1000-15 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Compressive Strength | 138 - 152 MPa | 20000 - 22000 psi | ASTM D695 |
Mar-Bal MB1000-PC Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Compressive Strength | 124 - 152 MPa | 18000 - 22000 psi | |
Bulk Molding Compounds BMC 100 Thermoset Polyester, GP BMC 100 is a high strength, low shrink general purpose molding compound. It can be supplied in bulk or extruded in pre-weighted slugs. Due to the excellent flow and controlled reactivity, BMC 100 is.. |
|||
Compressive Strength | 124 - 152 MPa | 18000 - 22000 psi | |
Bulk Molding Compounds BMC 102 Glass Filled Thermoset Polyester BMC 102 is a medium strength, glass fiber reinforced molding compound that meets Ford Specification ESF-M3D56-A. It can be supplied in bulk or extruded in pre-weighed slugs and is well suited for in.. |
|||
Compressive Strength | 110 - 152 MPa | 16000 - 22000 psi | |
Bulk Molding Compounds BMC 304 Automotive Grade Molding Compound BMC 304 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 304 can be coated using traditional or electrostatic coati.. |
|||
Compressive Strength | 124 - 152 MPa | 18000 - 22000 psi | |
Bulk Molding Compounds BMC 310 Cosmetic and Appliance Grade Compound BMC 310 is a cosmetic and appliance grade material with superior heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical app.. |
|||
Compressive Strength | 124 - 152 MPa | 18000 - 22000 psi | |
Bulk Molding Compounds BMC T15(F) High Strength Grade Molding Compound BMC T15F is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15F is well suited for injection, transfer or compression molding.. |
|||
Compressive Strength | 138 - 152 MPa | 20000 - 22000 psi | |
Bulk Molding Compounds BMC 1410 Electrical Grade BMC 1410 is a high-strength electrical grade material with excellent flammability resistance. In most applications, this material is competitive with SMC. Equal performance at a lower cost. Normally.. |
|||
Compressive Strength | 124 - 152 MPa | 18000 - 22000 psi | |
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel.. |
|||
Compressive Strength | 131 - 152 MPa | 19000 - 22000 psi | |
Bulk Molding Compounds BMC 810 General Purpose Molding Compound BMC 810 is a general purpose, very high strength compound suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reactivity and is wel.. |
|||
Compressive Strength | 138 - 152 MPa | 20000 - 22000 psi | |
Bulk Molding Compounds BMC SLC 2000 Glass Reinforced Polyester BMC SLC 2000 is a medium strength, low-cost, glass reinforced polyester compound with adjustable shrinkage. Ideal for circuit breakers, motor switch housings, fuse holders, brush holders, standoff i.. |
|||
Compressive Strength | 129 - 152 MPa | 18700 - 22000 psi | |
Bulk Molding Compounds BMC T40(18)-LS Die Casting Replacement Grade Molding Compound BMC T40(18)-LS is a low shrink compound designed as a direct replacement for aluminum die casting applications. T40(18)-LS is UL recognized. Excellent mechanical properties and dimensional stabili.. |