Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 8.00 - 12.0 MPa | 1160 - 1740 psi | Cold Crushing Strength |
Gouda Vuurvast FI 45-12 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 8.00 - 12.0 MPa | 1160 - 1740 psi | Cold Crushing Strength |
Gouda Vuurvast FI 55-11 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 8.00 - 12.0 MPa | 1160 - 1740 psi | Cold Crushing Strength |
Gouda Vuurvast FI 65-12 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 8.00 MPa | 1160 psi | Dried at 110°C (230°F) |
Skamol Group SKAMOCAST 14-105 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |
|||
Compressive Strength | 8.00 MPa @Time 360000 sec |
1160 psi @Time 100 hour |
|