Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 3500 MPa | 508000 psi | |
McDanel Advanced Ceramics SiAlON Information provided by McDanel Advanced Ceramic Technologies. |
|||
Compressive Strength | 3500 MPa | 508000 psi | ASTM C-773-88 / DIN 51067T1 |
CeramTec Rocar® S Silicon Carbide, SSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
Compressive Strength | 3500 MPa | 508000 psi | ASTM C-773-88 / DIN 51067T1 |
CeramTec Rocar® SiF Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
Compressive Strength | 3500 MPa | 508000 psi | DIN 51067T1 |
CeramTec Rocar® SiG Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
Compressive Strength | 3500 MPa | 508000 psi | ASTM C773 |
CoorsTek Direct Sintered Silicon Carbide, SC DS (SC-30, UltraSiC™) Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |