Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 260 MPa | 37700 psi | |
Saint-Gobain Micaver® Glass-Mica Electrical Insulator, Transfer Moldings Glass-mica compound that occupies a place between plastics and ceramics in terms of usage temperature. It can be molded and machined like plastics and has the mechanical properties (strength, hardn.. |
|||
Compressive Strength | 260 MPa | 37700 psi | ASTM D695 |
Sumitomo Bakelite North America E 8354A-1 Short Glass Fiber Reinforced Epoxy E 8354A-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito.. |
|||
Compressive Strength | 260 MPa | 37700 psi | ASTM D695 |
Sumitomo Bakelite North America E 8354A-2 Short Glass Fiber Reinforced Epoxy E 8354A-2 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito.. |
|||
Compressive Strength | 260 MPa | 37700 psi | ISO 604 |
Vyncolit X613 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Solenoid covers or automotive under-bonnet applications such as: water pumps, impeller.. |
|||
Compressive Strength | 260 MPa | 37700 psi | ISO 604 |
Vyncolit X7010 Novolac Phenolic Glass fiber reinforced molding compound with excellent mechanical and thermal properties.USES: Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Compressive Strength | 260 MPa | 37700 psi | ISO 604 |
Vyncolit X7012 Glass Fiber Reinforced Novolac Phenolic Novolac resin based, glass fiber and glass beads reinforced. High mechanical strength even at high temperatures in Long Life CoolantsInformation provided by Sumitomo Bak North America, Inc. |
|||
Compressive Strength | 260 MPa @Thickness >=5.00 mm |
37700 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola Etronax MMMF PTFE Phenolic, Cotton Fabric Reinforcement, Light Brown, Sheets Description: Friction reducing material consisting of phenolic resin with PTFE (Teflon®) and a very fine cotton fabric. Exclusively for mechanical applications. Very good dry run properties. Well s.. |
|||
Compressive Strength | 260 MPa @Treatment Temp. 150 °C, Time 3600 sec |
37700 psi @Treatment Temp. 302 °F, Time 1.00 hour |
ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope.. |
|||
Compressive Strength | 260 MPa @Temperature 23.0 °C |
37700 psi @Temperature 73.4 °F |
EN ISO 604 |
Ensinger TECASINT 5051 Polyimide, 30% Glass Fiber Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Compressive Strength | >= 260 MPa | >= 37700 psi | Ambient |
China-Yixing Longly Refractories Steatite Ceramics (High Frequency Porcelain) LONGLY's steatite ceramics (namely high frequency porcelain, strengthened porcelain, magnesia porcelain), molecular formula as MgO-SiO2, is pure white. Steatite is the appropriate option when good .. |
|||
Compressive Strength | >= 260 MPa | >= 37700 psi | Ambient |
China-Yixing Longly Refractories 75 Alumina Ceramic LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, .. |