Mechanical Properties Metric English Comments
Compressive Strength 248 MPa
36000 psi
Pyrotek TS-85 Thermoset Electrical Insulation Product (Nema Grade: L)
Linen reinforcement, Phenolic resin, Natural color. Good mechanical strength. Good machining qualities.Information provided by Pyrotek.
Compressive Strength 248 MPa
36000 psi
average
Potters Industries Ballotini® Impact Beads
Ballotini® impact beads are microspheres are used for precise metal finishing of parts. They offer an environmentally safe and cost effective method for metal surface cleaning and finishing. Coars..
Compressive Strength 248 MPa
36000 psi
ASTM D695
IDI Composites M-209 Thermoset Polyester, Sheet
MECHANICAL - Versatile family of compounds designed to meet a variety of mechanical, electro-mechanical, and corrosion applications. Outstanding structural properties at lowest possible costs.Data p..
Compressive Strength 248 MPa

@Thickness 12.7 mm
36000 psi

@Thickness 0.500 in
ASTM D695
Industrial Laminates/Norplex NP313 Cotton Fabric
Description: Canvas phenolic laminate with molybdenum disulfide lubricant. Mechanical properties slightly lower than NP310.Thickness Tested: 0.062", 0.125" & 0.500"
Compressive Strength 248 MPa

@Thickness 12.7 mm
36000 psi

@Thickness 0.500 in
ASTM D695
Industrial Laminates/Norplex NP319 Cotton Fabric Base Laminate
Description: Bleached canvas combined with phenolic resin and graphite lubricant. Better moisture resistance and machining characteristics than NP315.
Compressive Strength 248 MPa

@Thickness 12.7 mm
36000 psi

@Thickness 0.500 in
ASTM D695
Industrial Laminates/Norplex NP320E Cotton Fabric
Description: Similar to NP320 with improved moisture resistance. Suitable for electrical applications in moderate humidity conditions.Thickness Tested: 0.062", 0.125", and 0.500”
Compressive Strength 248 MPa

@Thickness 12.7 mm
36000 psi

@Thickness 0.500 in
ASTM D695
Industrial Laminates/Norplex NP347 Cotton Fabric
Description: Bleached canvas with high temperature phenolic resin with molybdenum disulfide lubricant. Low moisture absorption. Capable of 150°C continuous operation.Thickness Tested: 0.062", 0.1..
Compressive Strength 248 MPa
36000 psi
ASTM D-695
Glastic SG-200 Industrial Lift Magnet
Glastic Grade SG-200 high-strength and high-temperature laminates offer temperature ratings of up to 210°C. SG-200 is ideal for a wide variety of product applications requiring high-temperature ..
Compressive Strength 248 MPa
36000 psi
SGL Carbon Group EK 3245 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Compressive Strength 248 MPa
36000 psi
ISO 604
Sumitomo Bakelite North America RX® 640 Fiberglass Reinforced Phenolic Resole
RXÂ 640 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-5.Information supp..
Compressive Strength 248 MPa
36000 psi
ISO 604
Vyncolit Neopreg Kinel® SK61 L5G Glass Fiber Reinforced Molding Compound
Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particular suited for over molding..
Compressive Strength 248 MPa
36000 psi
Maximum Static Bearing Load
TriStar TriSteel AC Metal Backed PTFE Bearing System
Ultraflon 601 (AC) POM lined metal backed bearing system, boundary lubrication required, high PV. Ultraflon 601 POM Liner is a lubricant enhanced acetal material for use in lubricated or unlubricate..
Compressive Strength 248 MPa
36000 psi
Maximum Static Bearing Load
TriStar TriSteel PR Metal Backed PTFE Bearing System
Ultraflon 602e enhanced PTFE (PR) lined metal backed bearing , high speed reciprocating, self lubricating, high temperature and high load applications. Liner is designed specifically for high freque..
Compressive Strength 248 MPa
36000 psi
Maximum Static Bearing Load
TriStar TriSteel PT Metal Backed PTFE Bearing System
Ultraflon 602 (PT) PTFE lined metal backed bearing system, low friction, high PV, high speed sleeve, flange and thrust bearings, zero lube required, high operating temperature. Ultraflon 602 PTFE Li..
Copyright © lookpolymers.com All Rights Reserved