Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 220 MPa | 31900 psi | ASTM D695 |
PBI Performance Products Celazole® TF-60 C Carbon Fiber Reinforced Melt Processable Polybenzimidazole Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. .. |
|||
Compressive Strength | 220 MPa | 31900 psi | ASTM D695 |
PBI Performance Products Celazole® TF-60 V Glass Fiber Reinforced Melt Processable Polybenzimidazole Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. .. |
|||
Compressive Strength | 220 MPa | 31900 psi | Test specimen flat tested; ISO 604 |
Hexion Bakelite™ 460124 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a.. |
|||
Compressive Strength | 220 MPa | 31900 psi | Test specimen flat tested; ISO 604 |
Hexion Bakelite™ X30 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, reinforced with cotton and sisal fibers, increased notched impact strength.Application areas: Covers for electrical and electromagnetic devices.Information provided by Bak.. |
|||
Compressive Strength | 220 MPa | 31900 psi | ASTM D695 |
Sumitomo Bakelite North America E 9405H-1 Glass Filled Electrical Encapsulation Grade Epoxy E-9504H-1 is glass fiber filled epoxy molding compound designed for encapsulation of delicate electrical components as well as large coils. Excellent thermal shock, moldability, and retention of ele.. |
|||
Compressive Strength | 220 MPa | 31900 psi | ASTM D695 |
Sumitomo Bakelite Sumikon® PM-9501 Glass-Filled Phenolic, Compression Grade Sumikon PM-9501 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
Compressive Strength | 220 - 250 MPa | 31900 - 36300 psi | ISO 604 |
Vyncolit 4221 XB Novolac Phenolic Mineral and organic filled phenolic molding compound with good mechanical properties.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Compressive Strength | 220 MPa | 31900 psi | ISO 604 |
Vyncolit X6151 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Highest impact, high strain to failure, glycol resistant.USES: Water pumps and water pump .. |
|||
Compressive Strength | 220 - 260 MPa | 31900 - 37700 psi | ISO 604 |
Vyncolit X658 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties and a very good dimensional stability.USES: Complex precision parts.Information provided by .. |
|||
Compressive Strength | 220 - 240 MPa | 31900 - 34800 psi | ISO 604 |
Vyncolit X681 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubrica.. |
|||
Compressive Strength | 220 MPa @Temperature 23.0 °C, Time 86400 sec |
31900 psi @Temperature 73.4 °F, Time 24.0 hour |
50% RH, Axial; ISO 604; IEC/EN 61212-2 5.2 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Tubes Description: Mechanical and electrical applications. High mechanical strength. Self-extinguishing, halogen-free. Good resistance to chemicals.Information provided by Elektro-Isola |
|||
Compressive Strength | >= 220 MPa | >= 31900 psi | Perpendicular to laminations; IEC 1212-2 5.3 |
Hippe PF WV 201 Wood veneer Reinforced Phenolic Resin - Sheet Cross plied. Used in mechanical applications. Good mechanical properties.Information provided by Hippe. |
|||
Compressive Strength | >= 220 MPa | >= 31900 psi | Perpendicular to laminations; IEC 1212-2 5.3 |
Hippe PF WV 202 Wood veneer Reinforced Phenolic Resin - Sheet Cross plied. Used in mechanical and electrical applications. Good electrical properties under normal humidity.Information provided by Hippe. |
|||
Compressive Strength | 220 MPa | 31900 psi | |
Momentive Performance Materials Pyrolytic Boron Nitride (PBN) Coating High temperature protective coating for graphite.PBN has become the material of choice for compound semiconductor crystal growth and wafer processing. PBN coatings also seal and protect graphite fr.. |
|||
Compressive Strength | 220 MPa | 31900 psi | ASTM D695 |
Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Compression Grade Sumikon PM-6430 black Phenolic is a two stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional sta.. |
|||
Compressive Strength | 220 MPa | 31900 psi | ASTM D695 |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 50 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |