Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 169 MPa | 24500 psi | ASTM D695 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Compressive Strength | 169 MPa | 24500 psi | |
SGL Carbon Group Ridurid® V 1017 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Compressive Strength | 169 MPa | 24500 psi | ASTM D695 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Compressive Strength | 169 MPa | 24500 psi | ASTM D695 |
Sumitomo Bakelite North America RX® 525 Cellulose Reinforced Phenolic Novolac RX 525 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for parts requiring moderate toughness. It is designed to meet the requirements of ASTM D-594.. |
|||
Compressive Strength | 169 MPa | 24500 psi | ASTM D695 |
Plenco 6343 Phenolic, Granular, Compression Molded PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz.. |
|||
Compressive Strength | 169 MPa | 24500 psi | 10% Deformation; ASTM D695 |
Ensinger Tecapeek® XP-119G Compression Molded PEEK Compound, 10% Carbon Fiber with 5% Graphite Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Compressive Strength | 169 MPa | 24500 psi | 10% Deformation; ASTM D695 |
Ensinger Tecatron® XP-86 Compression Molded PPS Compound, with 40% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Compressive Strength | 169 MPa | 24500 psi | ASTM D695 |
Resinoid 2016 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |