Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | >= 14.5 MPa | >= 2100 psi | |
Engineered Syntactic Systems SF-30 Subsea Syntactic Void Filler SF-30 is a low cost, low density syntactic formulated to serve as a void filler for shallow water subsea applications. The material is provided as a three-part kit that is mixed and poured into any .. |
|||
Compressive Strength | 14.5 MPa @Temperature 1350 °C, Time 10800 sec |
2110 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories MRC-5 Blast Furnace Tap-Hole Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.5 MPa @Temperature 1260 °C |
2100 psi @Temperature 2300 °F |
Cold Crush Strength |
BNZ Materials Blazecrete 2600 Dense Castable Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as.. |
|||
Compressive Strength | 14.5 MPa @Treatment Temp. 540 °C |
2100 psi @Treatment Temp. 1000 °F |
Cold Crush Strength; Dried 104°C |
BNZ Materials Blazecrete 2600 Dense Castable Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as.. |