Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 10.0 MPa | 1450 psi | (C 165) |
Pyrotek Pyrite B-3 Refractory Board Pyrotek B-3 is a highly versatile calcium silicate board for use in a variety of machined shapes and general purpose applications. Among its uses, Pyrotek B-3 is established as the industry standar.. |
|||
Compressive Strength | 10.0 MPa | 1450 psi | 1% Yield Point; DIN 53454 |
Fluorseals PTFE Unfilled Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials. |
|||
Compressive Strength | 10.0 MPa | 1450 psi | EN 1094-5: 1995 |
Skamol Group Moler ROTOL Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Compressive Strength | 10.0 MPa @Time 36.0 sec |
1450 psi @Time 0.0100 hour |
|
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor.. |
|||
Compressive Strength | >= 10.0 MPa @Temperature 23.0 °C, Time 86400 sec |
>= 1450 psi @Temperature 73.4 °F, Time 24.0 hour |
@ 1% deformation, 140 Kg/cm<sup>2</sup>; ASTM D621 |
Adamas Adalon® 103 PTFE, 10% Carbon Filled Information provided by Adamas, HPM |
|||
Compressive Strength | >= 10.0 MPa @Temperature 23.0 °C, Time 86400 sec |
>= 1450 psi @Temperature 73.4 °F, Time 24.0 hour |
@ 1% deformation, 140 Kg/cm<sup>2</sup>; ASTM D621 |
Adamas Adalon® 118 PTFE, 23/2% Carbon/Graphite Filled Information provided by Adamas, HPM |
|||
Compressive Strength | 10.0 MPa | 1450 psi | measured on material fired at 370°C |
Pyrotek ISOCAST Insulating Refractory Castable Pyrotek's Isocast is a refractory castable based on phosphate bonded calcium silicate material. Isocast exhibits excellent thermal insulation characteristics and very good behavior with respec.. |
|||
Compressive Strength | 10.0 MPa | 1450 psi | |
Pyrotek Pyrocast SC-2600 Refractory Cast Parts Resistant to metal and flame abrasion, Pyrocast SC-2600 is the recommended castable refractory for applications such as filter box frames, burner tubes and troughs. The high purity silicon carbide .. |