Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco 10 WOLLASTOCOAT® Wollastonite Chemically treated grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco 400 WOLLASTOCOAT® Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco ASPECT® 3000 Wollastonite High aspect ratio grade. It is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. .. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco ASPECT® 4000 Wollastonite ASPECT 4000 is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive .. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco HARRP™ Coarse Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco M1250 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco M1250 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco M200 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco M325 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco MD1250 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco MD400 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco MG WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco NYAD® 1250 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco NYAD® 5000 WOLLASTOCOAT® Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco NYAD® M325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco NYAD® M400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco NYAD® MD200 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco NYAD® MD325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco NYAD® MD400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco NYAD® MG Wollastonite High aspect ratio grade. This grade is recommended for elastomer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinct.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco NYGLOS® 8 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco NYGLOS® M15 Wollastonite High aspect ratio grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal perf.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco NYGLOS® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco NYGLOS® M50 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco NYGLOS® MSTPO Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco NYGLOS® STPO Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco RRIMGLOS® II Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco ULTRAFIBRE® M30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco ULTRAFIBRE® 4W Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Tensile Strength | 2700 - 4100 MPa @Diameter 0.00300 - 0.150 mm |
392000 - 595000 psi @Diameter 0.000118 - 0.00591 in |
Fiber Strength |
Nyco ULTRAFIBRE® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |