Polymer Property : Tensile Strength = 9860 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 68.0 MPa
9860 psi
ASTM D638
SABIC Innovative Plastics EXTEM UH1006 TPI Blend
High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha..
Tensile Strength 68.0 MPa
9860 psi
ASTM D638
SABIC Innovative Plastics EXTEM UH1026 TPI Blend
High heat amorphous TPI Blend, Chemical Resistant, High Flow, IR-Transparent
Tensile Strength 68.0 MPa

@Thickness 4.00 mm,
Temperature 23.0 °C
9860 psi

@Thickness 0.157 in,
Temperature 73.4 °F
Injection Molded, 5.0 mm/min; ISO 527
PolyOne Bergamid™ B70 GK/Mi30 BK Polyamide 6 (Nylon 6)
Information provided by PolyOne
Tensile Strength 68.0 MPa
9860 psi
ASTM D638
Kolon SPESIN® KP513 PBT Alloy Resin
Excellent extrudable and SpinningApplications: Mono filamentInformation provided by API-Kolon.
Tensile Strength 68.0 MPa
9860 psi
ASTM D638
Kolon SPESIN® KP513UG PBT Alloy Resin
Extrudable, delusteringApplications: Mono filamentInformation provided by API-Kolon.
Tensile Strength 68.0 MPa
9860 psi
ISO 527
Premix Thermoplastics PRE-ELEC® PA 1411 Conductive Thermoplastic Compound
PRE-ELEC® PA 1411 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. PRE-ELEC® PA 1411 has a very low electrical resistivity. P..