Polymer Property : Tensile Strength = 838 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 5.78 MPa
838 psi
Silicone Property; Arlon SQA-TMS-008
Arlon 51981XA015 0.0150" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: 2.5 mil PolyethyleneThis data r..
Tensile Strength 5.78 MPa
838 psi
Silicone Property; ASTM D412
Arlon 51986R015 0.0165" (0.419 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater substrateAppearance: Red colo..
Tensile Strength 5.78 MPa
838 psi
Silicone Property; ASTM D412
Arlon 55986C028 0.0295" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: N/ASide 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave 2: LDPEThis data represents typical values for the pro..
Tensile Strength 5.78 MPa
838 psi
Silicone Property; ASTM D412
Arlon 56986XA028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flame Resistant-flexible heater substrateApp..
Tensile Strength 5.78 MPa
838 psi
Silicone Property; ASTM D412
Arlon 51986R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater substrateAppearance: Red colo..
Tensile Strength 5.78 MPa
838 psi
Silicone Property; ASTM D412
Arlon 51986RA020 0.020" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the producti..
Tensile Strength 5.78 MPa
838 psi
Silicone Property; ASTM D412
Arlon 51986XA015 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Gray silicone gum and rubber on fiberglass clo..
Tensile Strength 5.78 MPa
838 psi
Silicone Property; ASTM D412
Arlon 56986R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flame Resistant-flexible heater substrateApp..