Mechanical Properties Metric English Comments
Tensile Strength 5.72 MPa

@Strain 100 %
830 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible D80M0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 5.72 MPa

@Strain 100 %
830 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible XV3796 Polyvinyl Chloride, Flexible (PVC, Flexible)
All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high ..
Tensile Strength 5.72 MPa
830 psi
Silicone Property; ASTM D412
Arlon 514B12R006 0.006" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 1.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2116 FiberglassThis data represents typical values for the production material and should not be ..
Tensile Strength 5.72 MPa
830 psi
Silicone Property; ASTM D412
Arlon R34570R005 0.005" (0.127 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 1080 Style FiberglassThis data represents typical values for the production material. The data should no..
Tensile Strength 5.72 MPa
830 psi
Silicone Property; ASTM D412
Arlon R34572R005 0.005" (0.127 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 1080 Style FiberglassAppearance: Red silicone rubber on fiberglass clothThis data represents typical value..
Tensile Strength 5.72 MPa
830 psi
Silicone Property; ASTM D412
Arlon R37582R0055 0.0055" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 1.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2113 FiberglassThis data represents typical values for the production material and should not be ..
Tensile Strength 5.72 MPa
830 psi
Silicone Property; ASTM D412
Arlon R3758R0055 0.065" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 1.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2113 FiberglassThis data represents typical values for the production material and should not be ..
Tensile Strength 5.72 MPa
830 psi
Silicone Property; ASTM D412
Arlon R37652R0055 0.0055" (0.140 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 2113 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. ..
Copyright © lookpolymers.com All Rights Reserved