Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 56.0 MPa | 8120 psi | ASTM D638 |
Premix Premi-Glas® 3140-22 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 3140-22 is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves glass.. |
|||
Tensile Strength | 56.0 MPa | 8120 psi | ISO 527-2 |
NOVA Chemicals Dylark® 378P12 Glass Reinforced Engineering Resin Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim |
|||
Tensile Strength | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 136Q32 Nylon 6, Injection Molding Grade SAXAMID 136Q32 is a high impact-modified polyamide 6 injection-molding-grade.Information provided by SAX Polymers |
|||
Tensile Strength | 56.0 MPa | 8120 psi | |
Perstorp Compounds Akestra™ 110 Thermoplastic Copolyester Transparent sparkling glass-like appearance. Suitable for films, sheets, blow molding, foams and injection molding. It can be used as a polystyrene alternative for heat resistant thin wall contain.. |