Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 5.00 MPa | 725 psi | Cured State |
Palm Labs Adhesives TURBO FUSE SERIES 130 CLEAR FLEXIBLE (100 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 150 CLEAR FLEXIBLE advanced formula is designed to polymerize instantly by absorbing surface moisture. The produ.. |
|||
Tensile Strength | 5.00 MPa | 725 psi | ISO 37 |
Termopol Termoton® V2GA0065A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
Tensile Strength | 5.00 MPa | 725 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2620 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tensile Strength | 5.00 MPa @Strain 100 % |
725 psi @Strain 100 % |
ISO 37 |
BASF Elastollan B 80 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 5.00 MPa | 725 psi | 100; ISO 37 |
BASF Elastollan SP 883 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | 5.00 MPa @Strain 100 % |
725 psi @Strain 100 % |
ISO 37 |
BASF Elastollan S 85 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 5.00 MPa @Strain 20.0 % |
725 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan S 90 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 5.00 MPa | 725 psi | ISO 37 |
AlphaGary Evoprene™ G 992 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Tensile Strength | 5.00 MPa @Strain 300 % |
725 psi @Strain 300 % |
ISO 37 |
BASF Elastollan S 60 AWH TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |