Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 36.0 - 51.0 MPa | 5220 - 7400 psi | ASTM D638 |
Huntsman RenShape® SL 7820 Stereolithography Plastic RenShape® SL 7820 stereolithography material is a white, low viscosity and stable liquid that produces strong black models and prototypes with good surface fi nish and detail, and ABS-like appear.. |
|||
Tensile Strength | 36.0 MPa | 5220 psi | ASTM D412 |
GRECO ISOTHANE 3085AF Polyether TPU Resin ISOTHANE 3000F Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These pro.. |
|||
Tensile Strength | 36.0 MPa | 5220 psi | Weld; ASTM D638 |
Kuraray Genestarâ„¢ GN2332 Nylon, 33% Glass Filled High Flow V-0 Grade. Improves flow-ability in thin-walled parts. Used for components requiring high-flowability, such as 0.3 mm pitch connectors. |
|||
Tensile Strength | 35.99 MPa | 5220 psi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® ECO 12T95 Thermoplastic Polyurethane Type : Pearlthane® ECO 12T95 is a high performance bio-based thermoplastic polyurethane. With ca. 32% bio-based content.Main Application : Injection MouldingSpecial Features : Excellent mechanica.. |
|||
Tensile Strength | 36.0 MPa | 5220 psi | ASTM D412 |
GRECO ISOTHANE 1085AF Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject.. |
|||
Tensile Strength | 36.0 MPa | 5220 psi | 50 mm/min; ISO 527-1 |
Sax Polymers SAXALEN PPH319FX21 Polypropylene Homopolymer SAXALEN PPH319FX21 is a unfilled Polypropylene - Homopolymer intended for injection molding. It has flame retardant properties and suitable to produce thin-walled parts.Information provided by SAX P.. |
|||
Tensile Strength | 36.0 MPa | 5220 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1190 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 36.0 MPa | 5220 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1485RV Polyester Based TPU Good extrusion stability, high transparency, excellent mechanical propertiesInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 36.0 MPa @Strain 5.00 %, Temperature 23.0 °C |
5220 psi @Strain 5.00 %, Temperature 73.4 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 1000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | >= 36.0 MPa | >= 5220 psi | ISO 37 |
Austin Novel Materials Texalan® 685A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Strength | 36.0 - 48.0 MPa | 5220 - 6960 psi | DIN 53455 |
Isoflon ETFE Fluoropolymer material specifications.Information provided by Isoflon. |