Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina E 898-40/71-IS-RG Green PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina E818-18/99-CRM Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina 804-48/1-CRM Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina 809-36/467-CRM Brown PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina 818-08/39-Y-CRB Beige PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina 830-42/16-IS-RG Red PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina 835-42/14-IS-RG Red PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina 852-39/156-IS-RG Pink PVC Compound Non toxic PVC compound, recommended for blow molded bottles for cosmetics packaging.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina E 750-35/2-IS-SD-TR-LMP Ivory PVC Compound Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina E 80/278-IS-RG Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina E 800-10/194-Y-CRB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina E 800-35/1-Y-CRB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina E 805-48/1-IS-RG Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina E 806-21/10-IS-RG Coke PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina E 811-40/312-IS-RG Green PVC Compound Non toxic PVC compound, recommended for blow molding of bottles for alcoholic beverages.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina E 818-18/302-CRM Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina E 820-18/100-CR Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina E 830-18/99-CRM Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina E 836-10/176-CRA White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina E 854-18/99-CRB Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 34.3 MPa | 4980 psi | ASTM D638 |
Gromax PBT 2100-104B Product Description: PBT unreinforced flame-retarded injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellen.. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina E 844-10/176-CRB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina E 858-10/16-ERYA PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina E 898-02/160-IS-RG Yellow PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 34.3 MPa | 4980 psi | |
Taiwan Sheen Soon Sheenthane® A8630F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 34.3 MPa | 4980 psi | |
Taiwan Sheen Soon Sheenthane® A9312R Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 34.3 MPa | 4980 psi | |
Taiwan Sheen Soon Sheenthane® AH-585K Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmHotmelt adhesive gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 34.3 MPa | 4980 psi | |
Taiwan Sheen Soon Sheenthane® A9660 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina E 840-10/176-CRA White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 34.3 MPa | >= 4980 psi | ASTM D 638 |
Karina 802-35/1-IS-RG Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |